    How difficult is it to cut a thread on the end of a stainless steel rod?

    Will a regular set of dies, P&N or Chinese survive it or will it blunt the die?

    Following "Anorak Bob" I was considering changing some of the bars on machine handles to stainless.

    …..Live a Quiet Life & Work with your Hands

  2. #2
    Join Date
    Jan 2012
    Location
    Melbourne
    Posts
    149

    Default

    Should be OK if you use type 303, it will cut like mild steel and not workharden.
    I'm not familiar with other types.
    Neil

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Neil, Would 303 be your most common type or special order?
    …..Live a Quiet Life & Work with your Hands

  4. #4
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    I recently used a cheap Chinese die to cut a 3/8 NPT thread on some 316 stainless. I was surprised at the result. The thread was nice, clean and well formed. I used Trefolex and backed off after each half turn.

    From memory the die was carbon steel, not even HSS.

    Cheers,

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

  5. #5
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    If you want a reasonable (ie more than say25-50mm) length of thread, there's no way I'd cut it with a die. I'd go and buy a length of 316 allthread in the pitch I needed and weld, thread or otherwise butcher the gripping end to suit the task at hand.

    Some things simply are not worth doing.....

    PDW

  6. #6
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,540

    Default

    Certainly use Trefolex.

    Michael

  7. #7
    Join Date
    Feb 2013
    Location
    Laidley, SE Qld
    Posts
    1,038

    Default

    Depending on what I'm doing, sometimes I will single point a thread to 90% and finish off with a die.

  8. #8
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Quote Originally Posted by Michael G View Post
    Certainly use Trefolex.

    Michael

    Which one? Oil, Paste?
    …..Live a Quiet Life & Work with your Hands

  9. #9
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,540

    Default

    Paste

    M.

  10. #10
    Join Date
    Jan 2012
    Location
    Melbourne
    Posts
    149

    Default

    “……common type or special order? “
    We bought a couple of lengths from a supplier in Dandenong, off the shelf not special order. Can’t remember the supplier name, but I see 303 on a few local websites.
    FWIW, Metal Machinability comparison: http://www.engineeringtoolbox.com/ma...ls-d_1450.html

Similar Threads

  1. need help with threading
    By justron in forum METALWORK GENERAL
    Replies: 1
    Last Post: 2nd Sep 2014, 11:04 PM
  2. Threading again
    By morrisman in forum METALWORK GENERAL
    Replies: 18
    Last Post: 10th Dec 2011, 03:16 PM
  3. Threading Stainless Steel
    By funkychicken in forum METALWORK GENERAL
    Replies: 9
    Last Post: 15th Nov 2009, 02:11 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •