Thanks: 0
Likes: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 10 of 10
Thread: Threading Stainless
-
20th Dec 2014, 10:28 AM #1
Threading Stainless
How difficult is it to cut a thread on the end of a stainless steel rod?
Will a regular set of dies, P&N or Chinese survive it or will it blunt the die?
Following "Anorak Bob" I was considering changing some of the bars on machine handles to stainless.
…..Live a Quiet Life & Work with your Hands
-
20th Dec 2014, 12:17 PM #2Senior Member
- Join Date
- Jan 2012
- Location
- Melbourne
- Posts
- 149
Should be OK if you use type 303, it will cut like mild steel and not workharden.
I'm not familiar with other types.
Neil
-
20th Dec 2014, 12:29 PM #3
Neil, Would 303 be your most common type or special order?
…..Live a Quiet Life & Work with your Hands
-
20th Dec 2014, 12:33 PM #4Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
I recently used a cheap Chinese die to cut a 3/8 NPT thread on some 316 stainless. I was surprised at the result. The thread was nice, clean and well formed. I used Trefolex and backed off after each half turn.
From memory the die was carbon steel, not even HSS.
Cheers,
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
20th Dec 2014, 01:02 PM #5Most Valued Member
- Join Date
- Jun 2011
- Location
- Australia east coast
- Age
- 71
- Posts
- 2,713
If you want a reasonable (ie more than say25-50mm) length of thread, there's no way I'd cut it with a die. I'd go and buy a length of 316 allthread in the pitch I needed and weld, thread or otherwise butcher the gripping end to suit the task at hand.
Some things simply are not worth doing.....
PDW
-
20th Dec 2014, 03:16 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Certainly use Trefolex.
Michael
-
21st Dec 2014, 10:00 AM #7Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Depending on what I'm doing, sometimes I will single point a thread to 90% and finish off with a die.
-
21st Dec 2014, 10:14 AM #8
-
21st Dec 2014, 10:38 AM #9Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Paste
M.
-
21st Dec 2014, 09:43 PM #10Senior Member
- Join Date
- Jan 2012
- Location
- Melbourne
- Posts
- 149
“……common type or special order? “FWIW, Metal Machinability comparison: http://www.engineeringtoolbox.com/ma...ls-d_1450.html
We bought a couple of lengths from a supplier in Dandenong, off the shelf not special order. Can’t remember the supplier name, but I see 303 on a few local websites.
Similar Threads
-
need help with threading
By justron in forum METALWORK GENERALReplies: 1Last Post: 2nd Sep 2014, 11:04 PM -
Threading again
By morrisman in forum METALWORK GENERALReplies: 18Last Post: 10th Dec 2011, 03:16 PM -
Threading Stainless Steel
By funkychicken in forum METALWORK GENERALReplies: 9Last Post: 15th Nov 2009, 02:11 AM