    Hello all,

    I have just purchased a BS5A bandsaw from H&F and would like some advice on blades. I am not any experienced bandsaw user, and the machine only comes with a carbon blade. I understand bi-metal blades are the way to go but again I have no experience with them.
    The type of work I will be doing mainly consists of cutting 1020 steel around 1" solid round and square (model live steam locomotive), with the occasional larger cut.
    My questions are:
    Where is a good source for getting theses blades made?
    How many TPI should I order?
    Do I need evenly spaced teeth or variable pitch type blades?
    I am hoping some of you more experienced metal workers out there can steer me in the right direction with this.

    Thanks in advance,
    Ned

  2. #2
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    Hi Ned,

    When I purchased my S/H bandsaw it came with a 6/8 or a 8/12 multipich blade. A little too coarse for most of my anticipated use. I ened up buying a multipitch 10/14 M42 Bimetal blade from here:
    http://www.assetplant.com/epages/sho...th=/Shops/shop
    But there are many sellers on ebay too.

    It is a Roetgen brand (which meant nothing to me) but I can report that these bimetal blades are pretty good. While I don't use the machine EVERY day, I have used it quite a bit since I bought it and the blade really show no sign of blunting at this stage. I anticipate it will last me a number of years (assuming correct use and care). While for my machine it was not cheap at about $90 (3660x27mm) it will be a long time before I need to replace it.

    WRT the pitch or TPI, I would certainly look at a multipitch blade. I have been looking for a blade selection guide put out by Roentgen but I can't find it! I think as a guide you should allow between 2 - 6 teeth in the material at any one time. Any less and you run the risk of damaging or breaking off teeth, any more and you will find that the swarf cloggs the cut and jams the saw. I find that my 10/14 works really well for materials of similar size to your intended use and slightly larger with care. I always use coolant though.

    Good luck,

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Similar Threads

  1. Metal Bandsaw
    By ElDubya in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 14th Nov 2010, 11:18 PM
  2. scroll saw blades for metal
    By stonemason3 in forum METALWORK GENERAL
    Replies: 3
    Last Post: 7th Aug 2010, 06:57 PM
  3. Bi-metal bandsaw blades
    By Big Shed in forum METALWORK GENERAL
    Replies: 1
    Last Post: 7th May 2010, 07:09 PM
  4. Bi-Metal blades
    By Retromill in forum METALWORK GENERAL
    Replies: 7
    Last Post: 21st Dec 2006, 06:43 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •