Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 11 of 11
-
4th Dec 2013, 10:22 PM #1Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Machining clutch friction material
I need to cut out one of these clutch plates (7.5"OD x 4.5"ID x 5/16") from a square of friction facing material, its for a Howard cultivator, a low tech low speed application.
Ideally I would like to do it all on the rotary table with slot drills but I suspect the material will be very hard on the cutting edges.
Next best option is to use a scroll saw, it won't be as neat a job but scroll saw blades are very cheap.
Any thoughts?
-
4th Dec 2013, 10:26 PM #2Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
Looks like it could be made on a lathe, except for the 6 small holes.
Jordan
-
4th Dec 2013, 11:16 PM #3Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
However you end up doing it, I would think that serious thought needs to be given to dust collection, I may be wrong but I suspect that while friction material may no longer contain asbestos, the fibre reinforcement is probably still quite nasty and hazardous to health. A scroll saw would seem to be less of a dust producer and easier to set up with a shop vacuum than a mill with slot drills to do the machining, and also a lot easier to clean after the job was completed. You could even take the operation outside on a good day, and any dust missed by the shop-vac would be less of a problem than if it was in your workshop being recycled as you moved about. I agree that the material is likely to be hard on tooling, although the holes will probably need to be drilled - I imagine any attempt to punch them would likely shatter the material. A high pressure water jet may do it all, someone hopefully will chime in with the good oil. Regards,
Rob
-
5th Dec 2013, 05:27 AM #4Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 65
- Posts
- 3,103
Hi Bob,
Probably too late now but I had to make some plates for the line shafting clutch for the Jones and Shipman camelback drill at work.
Needless to say, plates weren't available so I got some tractor PTO clutch plates from Bareco and as they were 'in the ballpark' in size, they needed very little machining. This cut down on a lot of tool wear etc.
I used HSS (it's all I had) and wore a path to the grinder during subsequent re-sharpenings.
I attached them to a steel plate with a piece of pipe welded to the back for the 3 jaw chuck, and used a parting off tool to plunge cut towards the chuck to get the right diameters. Worked a treat.
Phil
-
5th Dec 2013, 07:57 AM #5Senior Member
- Join Date
- Dec 2010
- Location
- Syd
- Posts
- 492
Have cut down brake pads quite a few times with carbide. Dust, yeah, there's a bit, but I just use a paper mask and do a good clean up afterwards. Suppose a worry with something that appears to have no backing - like a pad - is how to prevent it fracturing, materials I have experience with are usually hard and brittle and you get the odd cut where you'll get a flake detaching instead of a clean one.
-
5th Dec 2013, 08:41 AM #6Most Valued Member
- Join Date
- Jun 2012
- Location
- SA
- Posts
- 1,649
The worst that can happen is you will fail.
But at least you tried.
-
6th Dec 2013, 11:27 AM #7Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
I've used angle grinders attached to lathe toolposts to machine clutch plate faces.
A vacuum cleaner nozzle placed close to the tool catches a lot of the dust.
Jordan
-
12th Dec 2013, 10:56 PM #8Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Thanks for the thoughts guys.
Tried the scroll saw but the clutch facing is way too hard for it.
Rotary table it will have to be, I have some cheap carbide slot mills coming that I won't mourn over if they get ruined.
I'll heed the dust control suggestions.
-
13th Dec 2013, 05:58 AM #9Senior Member
- Join Date
- Dec 2010
- Location
- Syd
- Posts
- 492
Thought there might have been an immediate need to do it. I know it might be less DIY and satisfying, the mobs who do this on a more regular basis water-jet the material, if there's some place nearby with the equipment, that's certainly one of the easier jobs.
-
9th Mar 2014, 10:36 PM #10Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Finally got back to this project. The good news is that cheap carbide slot drills - at least for the amount of cutting I did (1 circle at 110 dia and 1 at 190 dia) - cut clutch friction material without noticeably losing their sharpness.
I drilled the 6 x 7/16" holes with a HSS drill which lost its edge very quickly. It still kept cutting the soft ply and friction material OK, but the drill will need to be resharpened before it goes near metal again.
I sandwiched the clutch friction material between plywood to reduce the risk of it flaking or spalling, but now that I've done the job I don't know that I would worry about doing that next time.
-
9th Mar 2014, 11:05 PM #11Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,188
Just a word about those who want to machine stuff like this and think that a vacuum cleaner and face mask will make it safer.
If there is any chance that it has asbestos in it you need to know that asbestos fibres will pass straight through most vacuum cleaner filters and many masks.
Vacuum cleaners can make things worse because they make more fine dust out of bigger particles and they can quickly fill a shed up with fine dust that hangs around in the air for days and is almost impossible to clean up.
Even vacuum cleaners with the right sorts of filters often have leaks around damaged seals and cracks in the body of the cleaner and will continue to contaminate a shed very quickly.
If you have a vacuum cleaner that has been used to collect asbestos dust seriously consider disposing of it as it will continue to contaminate your shed for years, yes the whole vacuum cleaner and not just the filter. The motors become badly contaminated and cannot be cleaned all that easily
Vacuum cleaners and dust collectors that are located outside a shed are the way to go for this sort of work - and seriously consider disposing of the filters after you do the work as the filter will be forever contaminated and cleanup can not be assured.
Please also check the face mask is actually rated for asbestos (that's a P3 mask)