Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 15 of 15
Thread: The Comparator In Use
-
22nd Feb 2014, 07:02 PM #1.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
The Comparator In Use
The other day I received an email from Ray advising me that he had volunteered my services on PM. A bloke there had a Reilang oil can and was chasing the dimensions of some of its missing springs. Ray knew I had a similar oil can - http://www.woodworkforums.com/showth...61#post1620361
Upon dismantling the can I realised that whilst I could jam the jaws of my dial caliper between the coils to measure the wire, the reading varied depending on the pressure exerted on the wire. More importantly, I didn't want to damage or bend the springs. The answer was the Mitutoyo PJ250 Optical Comparator I had bought as an appetiser from fellow forum member Peter Fou. Appetiser because I bought it just before acquiring his wonderful tool and cutter grinder.
I have 0.005mm micrometer heads fitted ( thanks to Alan "C-47" ), the comparator came fitted with .0001" mics, so the measurements obtained would be a 10X improvement on the dial caliper. The micrometer heads have adjustable barrels allowing zeroing. So to measure the spring wire diameter it was nothing more difficult than bringing the wire into focus, aligning the cross hairs on one side, zeroing the mic and then winding the micrometer to move the cross hairs to the opposite side and reading the micrometer. The 0.29mm I had squeezed out of the caliper was actually 0.3mm.
I used the 20X lens, for more precise measurement with the tenth mics fitted, there is a 50X lens and for general close up sightseeing there is also a 10X lens. Sadly the latter lens' half reflection mirror has lost most of its mirroring. If my memory serves me correctly, the titanium (?) mirroring was/is applied by some vapour deposition process, hardly a back yard thing.
With a dial indicator of suitable sensitivity fitted to the, unfortunately not fitted, vertical indicator mount, accurate depth readings are also obtainable. Depth readings that would be pretty difficult to obtain otherwise.
The comparator is a neat bit of gear. Like centring scopes and auto collimators, not everyone's cup of tea but for those of us who have them, they add another dimension to our back shed explorations.
Bob.
-
22nd Feb 2014, 07:19 PM #2I used the 20X lens, for more precise measurement with the tenth mics fitted, there is a 50X lens and for general close up sightseeing there is also a 10X lens. Sadly the latter lens' half reflection mirror has lost most of its mirroring. If my memory serves me correctly, the titanium (?) mirroring was/is applied by some vapour deposition process, hardly a back yard thing.
Dean
-
22nd Feb 2014, 08:00 PM #3Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Every home should have at least one
Large telescopes use Aluminium coated surface mirrors. I cant say why they don't use silver though? maybe its easier to get off when its time for re-coating.
I wonder if you could replace the surface light and half mirrors with a ring of LEDS much like the Isoma. The light wouldn't be spot of vertical but as you have a ring of lights I'm not sure that would matter.. not sure that it wouldn't though lol
Nice pictures as always.
Stuart
-
22nd Feb 2014, 08:47 PM #4
-
22nd Feb 2014, 08:48 PM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
I seem to vaguely remember a chemistry experiment in high school that silvered a test tube (mix silver somethingate together with something else and silver precipitated out). Al probably replaced it as it was cheaper. If I had the space, PVD would be something I'd try setting up though as it leads to all sorts of fun combinations.
I replaced the light source in my comparator with a LED bulb and it does not seem to work as well. As good as LED are getting I think for a comparator the brighter the better.
Michael
-
22nd Feb 2014, 09:04 PM #6
Silver has a reflectivity of up to 99% compared to aluminium, which is around 90%. Gold gives the best reflectivity but produces a gold tint.
Here is a YouTube video of making glass mirrors with silver nitrate. I have not watched it. Just a comment to say maybe it is possible.
Dean
-
22nd Feb 2014, 09:11 PM #7.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
I don't know where the titanium came from Dean. Could be one of those getting old things. I had a bit of a dig on Google and mention was made of a thin silver coating allowing both light transmission and reflectance.
Mitutoyo offered a full reflection mirror which doesn't look too complicated. Stu had been experimenting with hard drive discs as mirrors for his prototype centring scope adaptors. I scrounged a hard drive from work and pulled it apart, mirrors abound!
Might be one of those afternoon gadget projects that runs into couple of weeks.
Bob
052 (Large).jpg
-
22nd Feb 2014, 09:14 PM #8Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
I doubt cost has much to do with it when we are talking about 8m telescope mirrors. If I recall correctly it takes 6g of Aluminium to coat the 8.2m VLT mirror.
Micheal are you talking about the profile light? I'd think that's more tricky than the surface light.
P.s. does Silver still beat Aluminium in infrared?
-
22nd Feb 2014, 09:21 PM #9Senior Member
- Join Date
- May 2010
- Location
- rural s.a.
- Posts
- 120
A place to start if you are looking at re-silvering. a.g. Thompson P/L. Tel. 1800 888466 I'm sure that they did vaccuum deposition in the 70's company has had owner changes since then I think. Hope this helps.
tinkera
-
22nd Feb 2014, 09:36 PM #10Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Hi Bob,
The thing that could be a problem with the side mirror(as your scan shows) it if the object isnt flat, you could end up with shadows. But if you have LEDS all the way around, that should improve things. More so on the 10x than the 20X as they will be further from the work. making the "off vertical" angle less. I dont have a 20x or 10x so I cant test it for you. Of course when Michael reports back about his LED I might be full of it
Stuart
-
22nd Feb 2014, 10:02 PM #11
Cost does not have a lot to do with the direct coatings of large telescope, mirrors but if you consider the huge number of smaller telescopes etc. around the world and then factor in the extra costs of safety handling and disposal of wastes it would make a difference.
According to Wikipedia, silver is effective right into the far infrared spectrum, but it does drop off considerably at about 550nm.
I had an idea to make a telescope, including lens at one stage. I was thinking around 8in to 12in. Nothing came of it. A mate at work has one which was home made by someone else. It is 16inches I believe. I think the lens was bought tho.
Bob,
Mitutoyo offered a full reflection mirror which doesn't look too complicated. Stu had been experimenting with hard drive discs as mirrors for his prototype centring scope adaptors. I scrounged a hard drive from work and pulled it apart, mirrors abound!
Might be one of those afternoon gadget projects that runs into couple of weeks.
Just as long as the afternoon project only occurs in the afternoon!
Dean
-
22nd Feb 2014, 10:09 PM #12Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Can I call a friend?
I have had this for several years but I'm yet to get it functional - I need to get a hood made and a stage for things to sit on. I think once that is done I may dispense with the light reflecting from the side and try illuminating directly from underneath.
Anyway - brightness -
P1020118 (Large).JPG
With the lights out at 9:30pm this is as bright as it gets (the exposure was 1/2.5 seconds from memory)
With the the lights on, it looks like this
P1020120 (Large).JPG
Michael
-
22nd Feb 2014, 10:31 PM #13Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Hi Dean,
I might have confused things, I meant that the cost of using silver wouldn't be a factor, so there must be some other good reason to use Aluminium. Maybe recoating is a pain or getting an even coating thickness?......I thought small scopes where silvered?
Google!
http://articles.adsabs.harvard.edu//...00018.000.html
Hi Michael,
That's a surface light.
Profile light comes from below, works much better but of course you can only see the edge/profile/silhouette.
I think the lens on my surface light is broken. I'll have a play tomorrow if I get a minute.
Stuart
-
22nd Feb 2014, 11:23 PM #14.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
I reckon the LEDs need to go MG. Mitutoyo at 8.15. Lights out. 1/6 at f3.2 No idea what the ISO setting is. For 79 bucks, who cares.
053 (Large).JPG
-
23rd Feb 2014, 12:12 AM #15
I knew you were the goto guy, who else has a Reilang Oil Can fetish AND an optical comparator...
That comparator is a nice bit of gear,
In similar vein we were discussing the other day, how I could get a micrometer stage under the Elmo video presenter.. maybe one day...
Ray
Similar Threads
-
Shipping damage and its repair on a Mitutoyo Optical Comparator's Protractor Screen.
By Anorak Bob in forum METALWORK GENERALReplies: 10Last Post: 24th Dec 2013, 12:42 PM -
Putting my optical comparator to work.
By Stustoys in forum METALWORK GENERALReplies: 13Last Post: 3rd Dec 2012, 12:03 PM -
Optical comparator
By Stustoys in forum METALWORK GENERALReplies: 2Last Post: 26th Jul 2012, 03:38 PM -
SOLD: Nikon optical comparator
By Greg Q in forum METALWORK - Machinery, Equipment, MARKETReplies: 6Last Post: 25th Jun 2012, 04:00 AM -
VICTORIA comparator stands and muir dails.
By azzrock in forum METALWORK - Machinery, Equipment, MARKETReplies: 4Last Post: 27th Apr 2012, 04:33 PM