Blacking As An Alternative to Bluing
Ray suggested the use of soot from a candle flame as a means of "colouring" an arbor to test its fit so I gave it a whirl this morning. I had been using bearing blue but with poor results either from a poor fit or poor application of the blue. Licking the flame across the metal results in a deposition of soot, the more licks the blacker. I tried three 30 taper arbors, my home made version, one from CTC and a Schaublin.
024 (Medium).JPG
Mine first. There is contact about two thirds of the way up the taper. I have some ISO 30 collets and their contact surface is about the same, so I won't fiddle with mine any further
021 (Medium).JPG 023 (Medium).JPG
The Chinese. It appears that the taper is hollow with contact at the ends only.
028 (Medium).JPG
And the Swiss. Pretty much uniform contact.
026 (Medium).JPG
I found this a lot easier than mucking around with blue. Thank you Ray.
Bob.
-
3rd Jan 2014, 10:24 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Bob, are you going to do the arbor I sent you with this method? I'm interested to know whether I've gained enough skills to be a Chinese machinist yet.
Michael
-
3rd Jan 2014, 11:55 PM #3Senior Member
- Join Date
- May 2010
- Location
- rural s.a.
- Posts
- 120
Hi Bob, something worth trying is lighting some camphor, easy to get from some moth/silver fish repellant from the local super market. Nice really black deposit.
tinkera
-
4th Jan 2014, 08:56 AM #4Most Valued Member
- Join Date
- Jun 2012
- Location
- SA
- Posts
- 1,649
Kero wick in a lantern would work well I suspect.
RobThe worst that can happen is you will fail.
But at least you tried.
-
4th Jan 2014, 12:18 PM #5Originally Posted by BT
I always associate lamp-blacking with leather aprons and flakey tobacco in tins, cloth caps, and running a lathe wearing a tie. Absolute precision craftsmanship and everything ruled by British Standards.
Ray
-
4th Jan 2014, 01:02 PM #6Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
According to the docco I saw Purdey is still much like that* and still use lamp black for final fitting of their actions.
Stuart
*with the odd CNC here and there
-
4th Jan 2014, 07:18 PM #7
-
6th Jan 2014, 08:32 AM #8Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
burning masking tape gives off a lot of soot
or you could you use a calcium carbide burner also
Similar Threads
-
My second attempt at steel bluing
By BobL in forum METALWORK GENERALReplies: 20Last Post: 4th Dec 2018, 02:25 PM -
Bluing a tapered shaft
By jack620 in forum METALWORK GENERALReplies: 20Last Post: 9th Apr 2013, 07:02 PM -
Blueing Blacking and Browning Formula Available
By hux in forum METALWORK GENERALReplies: 19Last Post: 17th Apr 2012, 09:46 AM -
Bluing
By bollie7 in forum METALWORK GENERALReplies: 1Last Post: 28th Apr 2009, 10:37 PM -
Metal bluing solution
By ohno in forum METALWORK GENERALReplies: 28Last Post: 16th Dec 2006, 08:00 PM