Thanks Thanks:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 6 of 6

Thread: Rolling copper

  1. #1
    Join Date
    May 2007
    Location
    Deception Bay / Brisbane
    Posts
    38

    Default Rolling copper

    Help from someone who knows what they are doing please.

    I am looking at sheet metal roller's and trying to determine what thickness copper they can roll. All the one's I looked at expressed the thickness they could bend when rolling mild steel.

    When you double the thickness of the material you require four times the force (everything else being the same), but the tensile strength of copper is about half that of mild steel.

    From this it looks like you can roll 1.5 times the thickness of copper instead of mild steel.

    Now if someone who knows what they are doing can tell me where I went wrong please.

    Thanks
    Dennis

  2. #2
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by denncarm View Post
    Help from someone who knows what they are doing please.

    I am looking at sheet metal roller's and trying to determine what thickness copper they can roll. All the one's I looked at expressed the thickness they could bend when rolling mild steel.

    When you double the thickness of the material you require four times the force (everything else being the same), but the tensile strength of copper is about half that of mild steel.

    From this it looks like you can roll 1.5 times the thickness of copper instead of mild steel.

    Now if someone who knows what they are doing can tell me where I went wrong please.

    Thanks
    Dennis
    annealed copper would be easiest to roll ...ie I dont think copper sheeting off the shelf is annealed meaning it would require more force....so this will add in another factor to consider

  3. #3
    Join Date
    May 2007
    Location
    Deception Bay / Brisbane
    Posts
    38

    Default

    Hi Eskimo

    To the best of my knowledge both the mild steel and copper tensile strength figures I got were for the un-annealed state but I am way out of my depth here.

    Thanks
    Dennis

  4. #4
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Quote Originally Posted by denncarm View Post
    I am looking at sheet metal roller's and trying to determine what thickness copper they can roll. All the one's I looked at expressed the thickness they could bend when rolling mild steel.

    When you double the thickness of the material you require four times the force (everything else being the same), but the tensile strength of copper is about half that of mild steel.

    From this it looks like you can roll 1.5 times the thickness of copper instead of mild steel.
    I make that to be roughly correct. To bend something you need to get the material to yield. Random numbers from the internet - yield of steel starts around 250Mpa, copper around 70Mpa. Stress in the outer layer of material is related to the thickness of the material cubed.
    Taking the cube root of (250/70) is approximately 1.5.
    So if you could roll 1mm steel in the rollers, you would expect to be able to roll 1.5mm copper.

    However,
    • Copper will work harden (get a higher tensile stress as it is manipulated), and
    • Yields of grades of copper vary with composition and supplied condition

    So while this is a reasonable rule of thumb, it may not always apply.

    Michael

  5. #5
    Join Date
    May 2007
    Location
    Deception Bay / Brisbane
    Posts
    38

    Default

    Thanks Michael

    All I was after was a rule of thumb, probably should have said it.

    Where I started from was rolling some 2.6mm thick copper for a boiler which means I would have to get a roller which would roll 1.6 mm of steel.

    Starting to get too expensive for the limited use it would get so I will just go to a firm with the machines.

    Thanks
    Dennis

  6. #6
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default copper

    what some one rolled you for your copper.
    aaron

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •