16th Jul 2013, 03:19 PM #46Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Hi PC,
I must have got something right as I went out to the shed I have 1.2mm on the cross-slide. I did a couple more light passes to "loosen" things up a little, then bored as above.
No change really.
As always hard to take pictures of blue.
I'd check my measurements then I think I'll just start knocking the compound around until things look better than they do now. I'd like to think it couldn't be far to go
Stuart
-
16th Jul 2013, 11:28 PM #47Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,088
Well I think I'm going to call it good.
It might be a little "the other way" now but its almost as good as my compound slide it seems. And I think if its going to be out its better to be out this way than the first way.
Call it half a tenth?1590 - YouTube
Stuart