Hi all,
Now i have my 2 taper pins made for tramming the Verniers head, one thing is clear. The head is not precisely trammed with the pins in! I have to pull the head off again and check there is not a tiny chip anywhere inbetween the mating surfaces, but i doubt it.
The pins are a 1:20 taper, and so far the only reamers i can find are for timber, they use 1:20 for stringed musical instrument tuning pegs....
The other option is to make a reamer from some silver steel, once hardened it should manage the 2 holes.
Has anyone seen or heard of a 1:20 reamer, or has any wisdom on making one i would be grateful.
Cheers,
Ew1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
14th May 2013, 09:08 PM #2
Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 70
- Posts
- 5,148
Do you have access to a grinder that can do tapers, if so what about using a drill bit ground to the taper required. To grind a tapered reamer from blank steel could be more work than necessary.
Either that or grind a spare reamer, you'll probably use it again somewhere!
Regards
Kryn
-
14th May 2013, 09:52 PM #3
Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,004
FWIW the taper on centreline of standard imperial taper pins is 1:24 and for metric taper pins it is 1:25
-
14th May 2013, 10:08 PM #4
Golden Member
- Join Date
- Oct 2012
- Location
- Australia
- Posts
- 621
Jarno Taper is 1:20
some examples here.
Helical Jarno Taper Reamers
-Josh
-
15th May 2013, 06:57 AM #5
Home Hobbist
- Join Date
- Aug 2008
- Location
- Oatley NSW
- Age
- 68
- Posts
- 257
Hi Ueee,
I have quite a number of Tapered Reamers and several No2's, send me your address and I will post one to you as I dont need them all.
Regards,
Keith_W.
-
15th May 2013, 08:42 PM #6
Thanks for the replies guys,
Its good to know the Jarno is 20:1 Josh, makes it a bit easier.
Bob, just to make it clear its 20:1 total taper, much steeper than the standard taper metric or imp.
Nothing more than bench and angle grinders here Kryn, but i like the drill bit idea.
Keith, that is a fantastic offer, once again a bigto the spirit of the forum! I think in need a #3 but i'll PM you about it.
Looking at the price of the Jarno reamers i might try making a D style reamer first.......
Cheers,
Ew1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
16th May 2013, 11:53 AM #7
Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
taper andle
would a 3 deg tapered drill work?
Similar Threads
-
5/8 tapered pin reamer
By azzrock in forum THE HERCUS AREAReplies: 11Last Post: 18th Nov 2010, 08:03 PM -
How do you Use a hand reamer
By rodm in forum METALWORK GENERALReplies: 11Last Post: 7th Feb 2010, 08:28 PM -
1MT Reamer
By Garell in forum METALWORK GENERALReplies: 3Last Post: 11th May 2006, 11:24 PM