8th Dec 2012, 08:31 PM #31
Gear oil
Hi
A misguided previous owner has filled the headstock on this lathe with automotive gear oil , looks like hypoid modern stuff, the gearbox has bronze bits in it. I flushed the headstock with kero, but any damage has already been done All seems Ok .. had a play and i am getting 40 to 830 rpm
-
18th Dec 2012, 08:39 AM #32Senior Member
- Join Date
- Jan 2009
- Location
- Captains Flat
- Age
- 71
- Posts
- 122
Headstock oil
Re oil for headstock and gearboxes..I was going to use "hypoid stuff" on my restored lathe ...what should I use when I get round to filling gearboxes up again?
David
-