Results 1 to 5 of 5
Thread: Another Mag transfer block
-
17th Nov 2012, 02:10 PM #1
Another Mag transfer block
Just another mag transfer block..
Nothing is ever quite as much fun as watching the shaper cast it's magic spell... Flattening a Mag Transfer Block - YouTube
Ready for finishing on the grinder..
Regards
Ray
-
17th Nov 2012, 04:48 PM #2
After the clean-up, Josh has finished grinding all faces square.
The purpose behind this transfer block is to be able to grind a 0.5 degree taper in the firmer chisels.
At the moment it's all square and parallel ... the next step is to grind a 0.5 degree taper..
The laminations are oven soldered as before, and the brass threaded rod is peened into a countersink on both ends.
Regards
Ray
-
17th Nov 2012, 08:27 PM #3
Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 58
- Posts
- 6,462
Ray, did you ever sort out the furnace brazing paste or are you still using solder?
Michael
-
17th Nov 2012, 10:47 PM #4
Hi Michael,
I'm still using the electronic type solder paste, it works pretty well, but I'm still interested in furnace brazing as a technique to develop further when I can get the right stuff to experiment with.
For this job the brass rods are probably enough just by themselves as far as strength goes. Soldering the parts together is probably a bit of overkill... not that I've ever shied away from overkill
Regards
Ray
-
19th Nov 2012, 10:36 PM #5
Most Valued Member
- Join Date
- Jul 2010
- Location
- Melbourne
- Posts
- 9,068
Nice one guys.
Going to you-tube took my tablets wireless over the limit and left me with my phone for the rest of the weekend :P
All finished yet?
Stuart
Similar Threads
-
Mag Transfer Block
By RayG in forum METALWORK GENERALReplies: 30Last Post: 23rd Oct 2012, 08:00 PM -
Transfer punches.
By aametalmaster in forum METALWORK GENERALReplies: 6Last Post: 17th Mar 2012, 08:46 AM -
Transfer screws and Transfer Punches