How big a hammer do you need?
Last weekend I was swinging my 16oz (450g) Sidchrome hickory handled ball pein hammer at a punch and suddenly had the head fly off in a ballistic arc on the back swing (handle broke inside the head). It was only 27 years old too (pause for a moment's silence).
Sidchrome may honour their lifetime guarantee, but in the mean time I need to get another hammer. Looking at what is available, there are steel handles, fibreglass handles, graphite handles, wooden handles and other stranger mixtures. Common weights seem to be 12oz, 16oz, 24oz, 32oz (and probably others exist too).
Hans anyone got any thoughts on what a good brand, weight and handle type is these days - I haven't bought one since I bought the kit with this one in it.
16oz seemed alright for most applications, although a little light for precision "really laying into something". Would I be better with say a 12oz for marking out and a 24oz for thumping?
Michael
-
14th Nov 2012, 09:59 PM #2
Diamond Member
- Join Date
- Aug 2006
- Location
- Melbourne
- Posts
- 1,014
I gave up on wooden handles years. The head flew off on mine a few times. It could easily knock someone out especially at work where there are usually a few people around.
I use fibreglass handles and havent had any issues with them yet. I use a 32 oz for pretty much everything at work, but a smaller one would probably be better for centre punching.
If anyone has any tips for keeping a wooden handle on I wouldn't mind knowing!
-
14th Nov 2012, 10:02 PM #3
Retro Phrenologist
- Join Date
- Oct 2009
- Location
- Springfield NSW
- Age
- 69
- Posts
- 75
I really hate to say this, but why not go over to the WOODTURNING forum and see if someone can make you a new hickory handle for your antique (?) hammer.
Yeah, I know it could be traumatic, but the blokes over there are really OK- they may not know their brass from their elbow joint but I'm sure they could help____________________________________________________________
there are only 10 types of people in the world. Those that understand binary arithmetic and those that don't.
-
14th Nov 2012, 10:50 PM #4
son of a blacksmith
- Join Date
- Jun 2011
- Location
- Roxby Downs Sth Aust
- Age
- 45
- Posts
- 205
-
14th Nov 2012, 11:32 PM #5
.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 70
- Posts
- 6,420
Michael,
I just slipped up to the shed to see what I have. My 16 oz ball pein is a hickory handled Blue Point. It's just a hammer. I have a nylon handled 24oz and a 12 oz leather handled Estwing. The 24 is great for heavy work.
I have a couple of bitty Blue Points that I use with prick punches and the optical centre punch.
My favourite is a 12 oz Cheney. It has an octagonal hickory handle that is slender and a pleasure to hold. The hammer is beautifully balanced. Cost me 5 bucks. Cheneys were the hammer when I was a kid. Held in the same regard as Disston Philadelphia saws. I had never laid eyes on a Cheney ball pein until I found mine.
I had a Plumb fibreglass claw hammer. Nice to use until, as a result of misuse, you start picking fibreglass out of your skin.
Go Hickory and American.
BT
-
15th Nov 2012, 07:05 AM #6
Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 58
- Posts
- 6,240
A new (replacement) handle would not be hard to find or fit, but at the moment I want to hear whether there is a better material out there.
Like Bob with his Cheney, when I was a teenager a carpenter that I respected swore by his Estwing and I've since had a secret longing for one. They do make a ball pein with a forged steel handle...
I agree that wood feels good to use but at the moment I'm concerned at how little time this handle lasted. I'm also thinking that a larger hammer for thumping and a smaller one for more precise tapping could be the go. I've seen ads for hammers with steel rod handles encased in rubber - billed as unbreakable. Could be good for handing out the odd bit of abuse.
Michael
-
15th Nov 2012, 07:16 AM #7
Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 64
- Posts
- 3,103
Hi Michael,
I have a 32 oz ball pein that has provided service under great duress since my apprenticeship. It still has the original wooden handle!
If the handle is fitted correctly they last and last and give great shock absorption. The key is 'well fitted' though. Kind of another skill that is leaving us.
Give me a wooden handle any day.
But then you know what I'm like
Phil
-
15th Nov 2012, 07:43 AM #8
Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,798
-
15th Nov 2012, 08:05 AM #9
Diamond Member
- Join Date
- Mar 2011
- Location
- Dural NSW
- Age
- 81
- Posts
- 1,193
Wooden Handles etc
Michael
Im with those who like the wooden handles.
Just checked my stock of ball pein hammers.
I have a 4oz 8oz 16oz 24oz 32oz
The first three are Australian Cyclone Forged hammers made in Wonthaggi Victoria the last 2 are USA & all still have the original wood handles.
I have owned all since new & date back 50 yrs plus,... (more silence)
Additional, one of my most useful hammers is a small homemade cross pein hardened hammer, of European design, about 4 oz.
It was made to primarily serve as a peening hammer for lightly peening hardened & ground thin steel sections for straightening, as in precision try square blade, plane blade, straightening etc. Introduces a compressive stress to the component & stretches the metal, with very accurate results.
I will attempt to get some photos.
regards
Bruce
ps In my woodworking hammers I like "Brades" English made, Warrington style (Cross Pein type)
These also have wooden handles.
-
15th Nov 2012, 08:19 AM #10
.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 70
- Posts
- 6,420
This will last a few lifetimes. Estwing Ball Peen Hammer 16oz 18478 | eBay
My 12oz leather handled Estwing was my go to hammer for twenty years. Then I found the Cheney.
As for carpentry Michael, I, like the bloke you know, swear by my Estwing forged claw. In my mind the best claw hammer made.
Bob
edit .. Bruce . You are back!
-
15th Nov 2012, 08:21 AM #11
son of a blacksmith
- Join Date
- Jun 2011
- Location
- Roxby Downs Sth Aust
- Age
- 45
- Posts
- 205
ever seen a blacksmith using a fibreglass handled hammer, must be a reason they only use wooden handles. when they break, linish the varnish off and use them for smoking fish or meat.
-
15th Nov 2012, 08:26 AM #12
Intermediate Member
- Join Date
- Jul 2008
- Location
- TAMWORTH, AUSTRALIA.
- Age
- 77
- Posts
- 30
G'day Michael, you might like to try this hammer!
Moonys 31.JPG
-
15th Nov 2012, 08:26 AM #13
All my hammers have timber handles, except 2 estwing steel and leather jobies. I have broken several handles whilst forging, but i just get a new one and fit it. I have always been wary of fiberglass handles, i have seen the results of one that has splintered and i never want it to happen to me. I also don't know how heat proof the fiberglass is which is important for use in the forge.....
The way Jordon described wedging the handle in is how i was taught, but the handle to head fit must be good first, no gaps etc....1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
15th Nov 2012, 10:15 AM #14
Diamond Member
- Join Date
- Mar 2011
- Location
- Dural NSW
- Age
- 81
- Posts
- 1,193
Returned
Bob
Yes, returned from Caravan & Camping trip up to Queensland & Moreton Island off Brisbane.
Have missed the Forum chatter.
I will give you a phone call soon. Whats the best time, when you dont have a paint brush in hand?
Regarding the Carpentry & claw hammer I would agree, the Estwing is the go.
Claw hammers get a lot of leverage loads, & the Estwing design is suberb.
regards
Bruce
-
15th Nov 2012, 11:42 AM #15
Member
- Join Date
- Nov 2007
- Location
- mid north coast NSW
- Posts
- 92
Hammer handles
I use wooden handled hammers that I fit myself, using both bought and self made handles. There are a lots of handleless hammer heads at the markets that are looking for a new owner, with careful selection you will find some of them are very well made, probably quite old and can (with patience) be found in good order and well worth rehandling. BWT walk away from "marketeer" handled hammers, not only are you getting a cheap second or third grade handle, the marketeer knows nothing about fitting handles and I think cares even less and your paying more than double for all his effort!!
Back to "modern" hammers with both fiberglass and wooden handles, you will find if you look closely that the head has been made with little or NO draught and is totally dependent on the glue to hold the head on the handle! Check out the draught in some of the old English made (ball pein) hammers, with a good handle and proper wedging they will last for years. I'm not against modern adhesives, some glued hammers may well be good enough for half my lifetime, but they can't be rehandled easily if at all! No doubt there will be a future (If not already?) law against self handled hammers in the work place!
Graeme