Hi
I'm not sure if this is the correct forum for this and I apologise for my lack of technical expertise.
I have an old Dawn No 7 quick release vice. I rescued it from a scrap heap a few years ago and it looks it is a goer. However there is one problem.
There is a what looks like a brass U bolt which allows for the quick release. The teeth have been worn down over the years and the thread slips. My question is, is it worth or
possible to have this repaired or should I just get the cast iron U bolt.
I have contacted Dawn in Melbourne and they have a cast iron replacement part for $50.00. I guess the brass part is designed to wear and not damage the screw.
I don't know how a cast iron U bolt would go it doesn't seem like it will work well.
TT
DSCF5277.JPGDSCF4181.JPGIMG_4677.JPGIMG_4678.JPGIMG_4681.jpgIMG_4683.jpgLearning to make big bits of wood smaller......
-
13th Nov 2012, 10:20 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Dawn wouldn't sell it if it was not going to work.
The CI will last longer than the brass.
Michael
-
13th Nov 2012, 10:33 PM #3
It looks like the thread is the same as my Record, which is a long way from a standard thread, be it ACME, square or 55/60 deg. If it is then the cost and time in trying to reproduce the angles involved would not be worth it. The CI will probably outlast you if you keep it well lubed.
1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
13th Nov 2012, 11:06 PM #4
Thanks for the input fellas
it looks like CI it is
Cheers