    This pic is from the Hendey factory pics series. I am wondering if this is a legitimate method of checking older worn lathe beds for a definite amount of wear . This method pictured is of a new machine being checked out .
    . alignment.jpg

  2. #2
    Join Date
    Oct 2011
    Location
    Sydney, NSW
    Posts
    1,249

    Default

    That's an interesting question. It must be accurate on a new machine - gives a good base/allowable reading (for the factory to pass it out). But you'd have to watch out for dents/dings etc on the bed of a older lathe.

    Ben

  3. #3
    Join Date
    May 2010
    Location
    Lower Lakes SA
    Age
    58
    Posts
    2,607

    Default

    I'm not really understanding that. But I have to assume Hendey knew more about making lathes than I ever will. Maybe one of our experts can help?

  4. #4
    Join Date
    Jul 2010
    Location
    Melbourne
    Posts
    9,088

    Default

    He is checking for parallel between the carriage and the tailstock ways right? Though he appears to be measuring on the flat on the top of the way. Which I guess would be ok to do at factory if you knew they were ground at the same time as the sides. No good once the machine has been used though.

    On second thoughts, if one assumes those two surfaces were parallel when it left the factory, as the top of the way gets little to no wear.... maybe you could use it as a test as any out of parallel would be wear in the carriage ways?

    Now where did those experts get to?

    Stuart

  5. #5
    Join Date
    Jul 2003
    Location
    The Fabulous Gold-plated Coast.
    Age
    69
    Posts
    2,251

    Default

    Its a problem in checking way allignment that the individual ways wear at different rates. Finding a reference surface from which to survey is the key to the problem. Often a lathe maker will grind a flat way that is recessed from the main ways, and hence left untouched by wear. I have seen lathes with the underside of the back way ground for use as a future reference.

    Greg
    It's all part of the service here at The House of Pain™

  6. #6
    Join Date
    Aug 2007
    Location
    Melbourne
    Age
    68
    Posts
    1,410

    Default

    Quote Originally Posted by morrisman View Post
    Hi

    This pic is from the Hendey factory pics series. I am wondering if this is a legitimate method of checking older worn lathe beds for a definite amount of wear . This method pictured is of a new machine being checked out .
    . alignment.jpg
    The guy has mounted the indicator on the saddle, and is measuring the front tailstock way whilst moving the saddle. I think this would be a legitimate method, even on a worn lathe. It is fair to assume that the headstock ways are not much worn close to the headstock, while the main ways would indeed be worn mainly close to the headstock. It may not tell you though, if the front and rear bedway have different wear. That you could better check by measuring a test bar between centers, both horizontally and vertically (of course, you would have to level the lathe first, or else you may confuse bed twist with wear).

    I am not sure, what exactly you want to do with the measures so aquired. I would be much more interested in the question, what sort of error does bed wear cause to my workpieces. That you check by cutting a long workpiece and measuring diameter along its length. Bed twist causes a linear error (taper), wear causes a non linear error (horglass shape) mostly close to the headstock. In practical use, bed wear is more a nuisance as you cannot adjust saddle to bed clearance anymore, it is sloppy towards the eadstock and binds towards the tailstock. Bed wear usually goes hand-in-hand with cross slide dovetail wear, the gib strip cannot be properly adjusted anymore, and the lathe may face convex instead of slightly concave.