    This arrived today

    The guys HIAB lifted it as if it was made out of paper .

    He ran the single sling around the spindle , behind the chuck YIKES ..I thought 1.5 ton taken on the spindle..But he said that's how they move them I wasnt convinced but didn't say anything ..I hope he didn't bend the spindle or damage the plain bearings


    The manual has GMH stamps on it . Acepted by GMH 6 Feb. 1948 central Plant & equipment

    3HP motor GE tag says 220/440 V 60 cycle

    Overall cond. is good. Bed looks nice . It's a 12 X30 model 12 speed . Its bloody big !

    MIKE

  2. #2
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,217

    Default

    Unlikely anything was damaged but picking a lathe up by the spindle is like getting yourself picked up by the balls....

    Looks a nice unit...
    Gold, the colour of choice for the discerning person.

  3. #3
    Join Date
    Mar 2008
    Location
    nowra
    Posts
    1,598

    Default

    Geez your quite a lathe collection nice lathe btw
    BETTER TO HAVE TOOLS YOU DON'T NEED THAN TO NEED TOOLS YOU DON'T HAVE

    Andre

  4. #4
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,723

    Default motor

    This is the motor tag

    I wonder if the resident motor guy on this forum ( RAY ?) can advise

    Will it run from single phase , without a VFD ?

    MIKE

  5. #5
    Join Date
    Jul 2010
    Location
    Melbourne
    Posts
    9,088

    Default

    Hi Mike,
    Congratulation. Sure looks the part!
    I'm with RC about lifting by the spindle but yeah it does seem to be done like that often.

    I cant imagine there is a single phase 440V motor, but Rays the man.

    Stuart

  6. #6
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    Mike,
    Congrats on the new machine, you will be turning more good steel into chips in no time.

    I'd never want to see a lathe hanging by its "balls" but i suppose i'd feel a bit better if it has plain bearings, although i'm guessing it doesnt.

    As for the motor it is probably good to run on either 440 or 220 three phase so no, you wouldn't be able to run it on single phase. I'm not sure about VDF's as i have 3 phase.....

    Was this one one ebay? It looks like i've seen pics of it before.

    Ewan

  7. #7
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Hi Mike,

    Nice solid looking machine, I've heard of people lifting lathes by the spindle, and don't really understand why they don't just put the slings under the bed and avoid risking damage. It's hardly any extra work.

    And yes, you'll need three phase power, or a VFD and wire the motor for 240 volt three phase. You get the added advantage of a bit of flexibility as far as speed control is concerned.

    Regards
    Ray

  8. #8
    Join Date
    Dec 2011
    Location
    South East Queensland, Australia
    Posts
    355

    Default

    She's beautiful, nice size.. Hope all is well and doesn't need to become a big project, unless you wanted that of course.
    Motor may very well be good for single phase, that would be a bonus. If it hasn't been run in a long time it would be a good idea to megger test it.

    Cheers.

    If I'm not right, then I'm wrong, I'll just go bend some more bananas.

  9. #9
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,723

    Default Ok

    Quote Originally Posted by Ueee View Post
    Mike,
    Congrats on the new machine, you will be turning more good steel into chips in no time.

    I'd never want to see a lathe hanging by its "balls" but i suppose i'd feel a bit better if it has plain bearings, although i'm guessing it doesnt.

    As for the motor it is probably good to run on either 440 or 220 three phase so no, you wouldn't be able to run it on single phase. I'm not sure about VDF's as i have 3 phase.....

    Was this one one ebay? It looks like i've seen pics of it before.

    Ewan
    Hi

    Thanks

    You won't believe it, but it has plain bearings . A Hendey oddity . They offered three different spindle bearings as an option. Plain, tapered roller or ball . This one is plain, it has oiling cups above each end of the spindle housing . The forward bearing is a double opposed type.

    Yes it was on EBAY . I was the only bidder . A good deal I thought, about half the price of a new same size asian lathe .

    Its capable of doing relieving work with attachments , some of which ame with it . It has a sub headstock too ... Another headstock for doing special jobs

    And, it has a threaded spindle end 2 and 3/4" 5 tpi ..no Camlock


    Mike

  10. #10
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    Quote Originally Posted by morrisman View Post

    Yes it was on EBAY . I was the only bidder . A good deal I thought, about half the price of a new same size asian lathe .


    And, it has a threaded spindle end 2 and 3/4" 5 tpi ..no Camlock
    Nice price! I just found it, i get emails for metal lathes....

    Not quite the same as the leblond spindle nose but close (2 5/8" 5tpi)
    Oh the joys of making backplates. At least you have a second lathe to make them on (or has the old one gone?)

    Also had a look at Tony's site, but mostly info on older Hendey's, nothing looking like yours.

    Ewan

  11. #11
    Join Date
    Oct 2008
    Location
    Wimmera
    Age
    51
    Posts
    369

    Default

    it must have been have a lathe follow you home day
    the hendy is very similar to the holbrook b model and t model

    cheers
    Harty

  12. #12
    Join Date
    Jul 2003
    Location
    The Fabulous Gold-plated Coast.
    Age
    69
    Posts
    2,251

    Default

    Liftting lathes by their spindles was a recent thread on PM. Some manufacturers actually illustrated it as the factory recommended technique. Not on my watch, but I guess that it's OK. Plain bearings are only a limitation when it comes to top speed...somethin less that 1500 will be your max, which will likely rule our carbide tooling, which should not be a big deal anyway.

    I admired that Hendey when it was listed and would have been a bidder if the space/time continuum was more friendly to one more unfinished project.

    Greg
    It's all part of the service here at The House of Pain™

  13. #13
    Join Date
    Oct 2008
    Location
    Wimmera
    Age
    51
    Posts
    369

    Default

    Hi mike
    they are a nice lathe bit light on with the cast though
    and id like to see more details of the relieving and spindle attachments

    here is what followed me home today
    Attachment 201367
    2500kg 15x36 with taper and relieving attachement (well part of it anyway)

    cheers
    Harty

  14. #14
    Join Date
    Jun 2011
    Location
    Adelaide
    Age
    27
    Posts
    248

    Default

    Congrats on your new toy!!
    How many lathes do you have now?
    Looks amazing love old lathes

    Cooper

  15. #15
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,723

    Default holbrook

    Quote Originally Posted by harty69 View Post
    Hi mike
    they are a nice lathe bit light on with the cast though
    and id like to see more details of the relieving and spindle attachments

    here is what followed me home today
    Attachment 201367
    2500kg 15x36 with taper and relieving attachement (well part of it anyway)

    cheers
    Harty

    Yes , seems like we have some kinda problem, lathes are addictive

    That Holbrook is a monstor . It is about 1/3 rd as heavy again as this Hendey I bought your truck looks rather down on the back springs LOL

    I got a shock looking at the Norton gear box label, on this Hendey . Its all written in French the tpi on the plate are in very odd metric increments . Holy cow I thought to myself ' . GOD is this a metric lathe .... But the leadscrew is 6 TPI , no doubt about it ... The agents tag on the bed is a company in PARIS , France ..How did GMH get hold of it ?

Page 1 of 7 123456 ... LastLast

Similar Threads

  1. Hendey 12 X 30 lathe
    By morrisman in forum METALWORK GENERAL
    Replies: 8
    Last Post: 29th Feb 2012, 12:51 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •