How to tightly hold a bundle of small steel rods
Im making another pair of these hand carders for SQMBO.
These ones are made from 2mm regular steel TIG welding rods
IMG_4685.jpg
This time I'm using 3mm TSS rods.
Cutting 48 equal length rods is pretty monotonous. They don't need to be a specific length but they should all be the same, so I rough cut them on my thin kerf abrasive table saw and was looking for a way to hold a bundle together to hold them all even at one end so's I could sanded the other end all to the same length.
Tried zip ties - SS was too slippery, Then I tried using a collet in a collect chuck/block.
Get the all levelled up like this
colletEnd.JPG
And grind the other end on a disc sander like this.
You'll notice one is still short - that's just a spare to help the others sit tight in the collet - its not going to be used in the final pieces.
groundend.JPG
Now have to sharpen one end, bend the sharpened tips, and make up some handles.
-
15th Sep 2021, 05:48 AM #2Intermediate Member
- Join Date
- Jul 2021
- Location
- Europe
- Age
- 30
- Posts
- 36
if you need to produce a lot of equal lenght rods, fast, you can make your own angle grinder stand with fitting vise, or really just run it through a mounted pipe thats about 10mm off the table/plate you mount it on
we cut up M20 threaded rods for concrete walls that gets epoxied into the ground, and i finally had enough of them breaking the sawblade and occupying out band saw for a whole day cutting out a handful of these rods.
with a thin cutting disc you will go through 10mm rod in seconds, you can just weld some angle iron at the required distance and its quite swift to make your own angle grinder stand, otherwise maybe 20 dollars to buy one, cutting up whole lenghts of metal rods takes me very short time, i dont even clamp it in place, once the cutting disc bites it stays in place, i just keep my left hand on the rod and guide the angle grinder down with right hand with a metal rod sitting in the angle grinder handle to extend it and work against the spring keeping the angle grinder back when i let go
for my device i decided to shape some holeplate to fit my angle grinder, then a nut/bolt open/close mechanism, takes very little time to attach my angle grinder, its ready to go in less than 60 seconds and what would take maybe hours on the bandsaw- and ruining the sawblade in the process takes me maybe 15 minutes
Similar Threads
-
Tig brazing rods v's Oxy rods. Any difference?
By Zumanity in forum WELDINGReplies: 8Last Post: 13th Mar 2020, 09:21 AM -
which steel for small jeweller roller?
By Alex_Campili in forum JEWELLERYReplies: 2Last Post: 12th Nov 2017, 12:44 AM -
GP arc mild steel welding rods for teaching
By Paul M D in forum WELDINGReplies: 9Last Post: 18th Jun 2016, 12:49 AM -
Small steel Engineering job please
By seriph1 in forum METALWORK GENERALReplies: 19Last Post: 25th Feb 2016, 09:47 PM -
Question On Welding Rods and RHS Steel
By mattwolf in forum WELDINGReplies: 1Last Post: 29th Jul 2009, 10:11 PM