    Hello, this is my first proper post here though I've been lurking for a while.

    A few years back I bought a pair of TCT blades for the Ozito plunge saw (24T x 89 mm x 10 mm, about 1/16 kerf) for a project that never happened. Today I though I'd try one as a slitting saw to cut 25 mm deep slits in 8 mm mild steel.

    Worked like a charm. I mounted it on my home-made 10mm arbor (18 mm OD) and stuck it in a collet on the old mill/drill. After a little experimentation I found it cut happily at about 250 RPM lubricated with squirts of WD40.

    Given the tolerances here and there most of the teeth weren't doing any work, so between slits I loosened the fixing bolt on the arbor and rotated the blade a bit in the hope of evening the wear. (The arbor is home made, 16 mm OD at the business end.)

    At about $13 for a pack of two these blades seem like a good value where precise thickness isn't an issue.

  2. #2
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,475

    Default

    Quote Originally Posted by Giordiannetto View Post
    Hello, this is my first proper post here though I've been lurking for a while.

    A few years back I bought a pair of TCT blades for the Ozito plunge saw (24T x 89 mm x 10 mm, about 1/16 kerf) for a project that never happened. Today I though I'd try one as a slitting saw to cut 25 mm deep slits in 8 mm mild steel.

    Worked like a charm. I mounted it on my home-made 10mm arbor (18 mm OD) and stuck it in a collet on the old mill/drill. After a little experimentation I found it cut happily at about 250 RPM lubricated with squirts of WD40.

    Given the tolerances here and there most of the teeth weren't doing any work, so between slits I loosened the fixing bolt on the arbor and rotated the blade a bit in the hope of evening the wear. (The arbor is home made, 16 mm OD at the business end.)

    At about $13 for a pack of two these blades seem like a good value where precise thickness isn't an issue.
    Hi, I've been doing a similar thing with those cheap 125 mm TCT saw blade out of Aldi and Lidl ! Very good value. I've found that the blades are quite well centred and don't wobble up and down making the cut wider than it needs to be. I've used mine on both the lathe and mill, but at 450 rpm the drill press is a bit too fast for safe working.
    Best Regards:
    Baron J.

  3. #3
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    Pictures or it never happened.
    Gold, the colour of choice for the discerning person.

Similar Threads

  1. Cheap Protection from Super Cheap.
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 4
    Last Post: 30th Apr 2014, 12:01 AM
  2. Slitting saw keys
    By Ueee in forum METALWORK GENERAL
    Replies: 6
    Last Post: 17th Feb 2013, 11:45 PM
  3. Slitting Saw Holders
    By Jors in forum METALWORK GENERAL
    Replies: 3
    Last Post: 10th Dec 2012, 09:47 AM
  4. Cheap vices at Super Cheap Auto
    By LordBug in forum METALWORK GENERAL
    Replies: 19
    Last Post: 5th Jun 2011, 01:14 AM
  5. MT-3 slitting saw arbors
    By hitachi230 in forum METALWORK GENERAL
    Replies: 7
    Last Post: 3rd Jun 2008, 12:16 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •