    To get a nice consistent point on my Centre Punches, I put them in the DP at around 600 rpm, and use a small angle grinder held at the correct angle, for a short period.
    Taking off the mushroom head can also be done on the DP, with good results.
    Kryn
    To grow old is mandatory, growing up is optional.

  2. #2
    Join Date
    Oct 2010
    Location
    melbourne, laverton
    Posts
    1,910

    Default

    Cool Merrill try that

  3. #3
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Both my spring loaded centre punches won't run true in my drill press, while the non-spring loaded ones have square shanks

  4. #4
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Quote Originally Posted by BobL View Post
    Both my spring loaded centre punches won't run true in my drill press, while the non-spring loaded ones have square shanks
    Hi Bob, Guys,

    The spring loaded ones, I remove the punch, its also easy to make new ones for them !

    I sharpen my centre punches in the lathe using a Dremel in the tool post. About the only time that I've used the drill press is to hold a short length of silver steel when I've already made the point by turning and I'm heating it to harden the tip. I spin the silver steel and then get it red with a cooks torch, then plunge into a tin of oil ! Usually the cooking oil that the wife throws out of the chip pan, smells of chips... mmm. I've made several transfer punches this way.
    Best Regards:
    Baron J.

  5. #5
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Useful tip about removing the tip on a spring loaded punch to sharpen it.

    To sharpen tips on stuff that fits in a cordless drill I spin the tips against an unsupported part of a Linisher belt.
    Sometimes I sharpen TIG tips against a diamond wheel.
    The tips on the tines of this wool carding comb were made this way.
    The tines are pieces of TIG rod

    IMG_4685.jpg
    Which is why I wanted to get the all the same length.
    colletEnd.JPG
    Attached Images Attached Images

  6. #6
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    Note that grinding should be parallel to the axis of the punch, not across it.

  7. #7
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by nadroj View Post
    Note that grinding should be parallel to the axis of the punch, not across it.
    I can’t picture what that means. And even if I could, I don’t think I’d understand why. Can you elaborate please Jordan?
    Chris

  8. #8
    Join Date
    Nov 2008
    Location
    North Brisbane. Qld. Australia
    Age
    70
    Posts
    1,513

    Default

    Quote Originally Posted by jack620 View Post
    I can’t picture what that means. And even if I could, I don’t think I’d understand why. Can you elaborate please Jordan?
    Grinding along shank toward tip I assume. Didn't know that 'till now. Thanks.
    Nev.

  9. #9
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by nadroj View Post
    Note that grinding should be parallel to the axis of the punch, not across it.
    I grind/shape across a coarser belt first, and if possible also use an unsupported part of the belt to avoid getting a flat. Then switch to a finer belt along the line of the work

  10. #10
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    I read it in a few different places, that grinding a centre punch should be such that any grooves (tiny but there) should be towards the conical tip.
    I thinks it's to minimise the effect of any stress risers weakening the tip.

  11. #11
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Guys,

    I have a centre punch that does not have a conical point !

    Instead it has a three sided pyramid shaped point and is quite sharp compared to the conical point ones. Its also very easy to find the intersection of scribed lines with it. You can easily feel the scribe mark.
    Best Regards:
    Baron J.

  12. #12
    Join Date
    Mar 2013
    Location
    Mt Pleasant SA
    Posts
    126

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Guys,

    I have a centre punch that does not have a conical point !

    Instead it has a three sided pyramid shaped point and is quite sharp compared to the conical point ones. Its also very easy to find the intersection of scribed lines with it. You can easily feel the scribe mark.
    Meant for centre punching stainless steel .. as are 4 sided. Theory is it's easier for the drill point to cut thro' the work hardening.

  13. #13
    Join Date
    May 2020
    Location
    s.w. sydney
    Posts
    53

    Default

    Quote Originally Posted by KBs PensNmore View Post
    To get a nice consistent point on my Centre Punches
    Kryn
    just curious, why does it need to be a nice consistent point ?
    i sharpen drills 3mm to 60mm on a bench grinder, whats wrong with a bench grinder?
    cheers

  14. #14
    Join Date
    Aug 2008
    Location
    Melbourne
    Age
    34
    Posts
    1,080

    Default

    You want to make it consistent so it's easier to line up on your scribe lines. Nothing wrong with a bench grinder at all
    Gear cutting specialists and general engineers www.hardmanbros.com.au
    Fine pitch gear cutting from 0.1 Module www.rigear.com.au

  15. #15
    Join Date
    May 2020
    Location
    s.w. sydney
    Posts
    53

    Default

    Quote Originally Posted by elanjacobs View Post
    You want to make it consistent so it's easier to line up on your scribe lines. Nothing wrong with a bench grinder at all
    i think i understand, i would call it a "fine" point

Page 1 of 2 12 LastLast

Similar Threads

  1. Automatic Centre Punch
    By Twisted Tenon in forum METALWORK GENERAL
    Replies: 11
    Last Post: 27th Sep 2017, 01:27 PM
  2. Sharpening Spring Loaded Centre Punch
    By Fuzzie in forum METALWORK GENERAL
    Replies: 7
    Last Post: 29th Nov 2015, 04:06 PM
  3. Optical centre punch for 'simonl'
    By Steamwhisperer in forum METALWORK GENERAL
    Replies: 53
    Last Post: 30th Aug 2012, 06:11 PM
  4. Optical centre punch
    By morrisman in forum METALWORK GENERAL
    Replies: 5
    Last Post: 9th Aug 2012, 01:16 AM
  5. Centre punch mark magnifer
    By neksmerj in forum METALWORK GENERAL
    Replies: 15
    Last Post: 18th Jul 2007, 01:59 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •