Results 1 to 5 of 5
  1. #1
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Thumbs up Brass tip in Grubscrew !

    Hi Guys,

    Just passing on a tip given to me by Kryn.

    A tip I picked sometime ago, was to drill the end of the grub screw and place the little brass screws from electrical fittings in, so they don't bite into the shaft, as even without serrations, they still bite into it. DAMHIKT.

    Drill the hole slightly smaller than the shaft of the screw and hammer them in.

    Kryn
    Thanks Kryn
    Best Regards:
    Baron J.

  2. #2
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Another method I've seen, but not tried, is to grind a nice clean flat on the tip of the grub screw then braze a big blob of bronze onto the screw. Then turn the blob down to something more pretty.
    Chris

  3. #3
    Join Date
    Aug 2008
    Location
    Adelaide
    Age
    68
    Posts
    1,374

    Default

    Quote Originally Posted by jack620 View Post
    Another method I've seen, but not tried, is to grind a nice clean flat on the tip of the grub screw then braze a big blob of bronze onto the screw. Then turn the blob down to something more pretty.
    This works well, especially using TIG brazing as the control over the size of the deposit is excellent. With practice you can get it such that no final machining is required.

  4. #4
    Join Date
    Oct 2008
    Location
    Cairns, Q
    Posts
    666

    Default

    Quote Originally Posted by jack620 View Post
    Another method I've seen, but not tried, is to grind a nice clean flat on the tip of the grub screw then braze a big blob of bronze onto the screw. Then turn the blob down to something more pretty.
    I have often done this - not a big blob though - only a small amount. If the screw is long enough I screw an old button die or die nut onto the screw first. Then when you unscrew the die it cuts a perfectly aligned thread in the bronze, and no further machining is usually required.

    Frank.

  5. #5
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,673

    Default

    Tried the TIG and button die method today and it worked well.

    I also put the button die in a handle and used the earth clamp to hold it to the table which made it really easy to get it in a good position, and great earth contact.

    I forgot to grab a photo of the die and handle setup but here is the end result.



    Steve

Similar Threads

  1. what rods for thin brass to brass ??
    By Mathuranatha in forum WELDING
    Replies: 7
    Last Post: 23rd Nov 2020, 08:17 PM
  2. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  3. 5/16 Brass
    By rogerbaker in forum METALWORK GENERAL
    Replies: 3
    Last Post: 11th Nov 2012, 10:57 PM
  4. brass
    By tanii51 in forum METALWORK GENERAL
    Replies: 3
    Last Post: 22nd Aug 2009, 09:21 PM
  5. Brass on Brass
    By funkychicken in forum METALWORK GENERAL
    Replies: 10
    Last Post: 24th Mar 2009, 09:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •