No googling, The info comes from a set of 50 year old metal working books that an old techie gave me at work about 10 years ago, and the documents and notes from a blacksmith course I attended 5 years ago.
Whether a steel is oil, air or water quenched doesn't have much to do with carbon content.
WI and O1 are water and oil quenching steels respectively, and have very similar carbon contents.
A2 (similar Carbon content to both W1 and O1) and is preferably air quenched.
M2 has the narrowest range of Carbon content that is inside the ranges for W1, O1 and A2, and can be brine, oil or air quenched.
Hardening to depth (case hardening) has been done since Roman times.
The method you refer to above about wrapping metal in hair and bone to infuse C into metal only works for a shallow depth is an example. Teh Carbon from the padding materials does not penetrate far thick pieces of steel no matter how long you leave it.
Since medieval times serious blacksmiths developed special case hardening powders and these are widely available - you might like to try google to see how widely available they are?
One of the members on these forums has been selling this stuff and was giving away small samples at one of the scraping class meets in 2014?
-
23rd Mar 2018, 02:38 PM #17Banned
- Join Date
- Jan 2018
- Location
- Aldinga Beach.
- Age
- 73
- Posts
- 148
Case hardening? Who the devil is talking about case hardening, certainly not me. Case hardening would have worked real well on swords wouldn't it? Case hardening is not hardening to depth, totally different processes. Case hardening is as its name suggests adding a layer of hard material. Carbon infusion is also as it suggests, carbon is infused into the metal.
I google all the time, but mostly I know what I know not from reading books or googling but from actual experience. W1, W2, etc,means beans to me.
Some useless info: Old samurai swords were made by wrapping carbon steel around a softer steel this is what gave the swords their fine edges and toughness. I have read that today's swordsmiths have difficulty in replicating these swords.
More useless info: Damascus steel was made by heating very low carbon steel, sprinkling it with very small pieces of high carbon steel, folding and beating over and over. This is what gives Damascus steel it's pattern or what looks like grain. It was said that a Damascus steel sword could be bent in a circle so tip touched pommel and when released would spring back to it's original shape - straight. Whoever was able to bend a sword like that would certainly put Arny to shame! Damascus steel knives are available on ebay should anyone wish to try them.
I'm sure someone will feel the need to add corrections with dates, percentages, etc. Just more useless information, but entertaining nevertheless!
-
23rd Mar 2018, 09:04 PM #18Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
. . . W1, W2, etc,means beans to me.
-
23rd Mar 2018, 09:33 PM #19Diamond Member
- Join Date
- Oct 2008
- Location
- N.W.Tasmania
- Posts
- 1,407
I'm with BobL on this one Onanonanon, you may not have mentioned the term "case hardening", but you have certainly mentioned the process. Case hardening refers to a process not where an extra layer of hard material is added, but a thin outer layer has carbon infused into it making it a higher carbon steel, and so capable of being hardened by quenching into some quenching medium, be it water, brine, oil, air or any other suitable quenching medium. The process you spoke of using hair and bone fragments wrapped around the workpiece and heated in the relative absence of oxygen, followed by quenching, is one process which will case harden suitable steels, but I have no knowledge of it being suitable or otherwise for the manufacture of sword blades. I would think that if there was a suitable steel for case hardening, which was tough, like a spring steel for instance, it could work, but there may be difficulties obtaining a suitably tough springy steel which could still be case hardened, I simply don't know.
-
23rd Mar 2018, 10:22 PM #20Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Cheers RT.
Modern case hardening is indeed usually just a very shallow process but look up the Wikipedia entry for "Case hardening", under the "historical section of case hardening" it states;
The traditional method of applying the carbon to the surface of the iron involved packing the iron in a mixture of ground bone and charcoal or a combination of leather, hooves, salt and urine, all inside a well-sealed box. This carburizing package is then heated to a high temperature but still under the melting point of the iron and left at that temperature for a length of time. The longer the package is held at the high temperature, the deeper the carbon will diffuse into the surface. Different depths of hardening are desirable for different purposes: sharp tools need deep hardening to allow grinding and resharpening without exposing the soft core, while machine parts like gears might need only shallow hardening for increased wear resistance.
There were many other methods to obtain the optimum spatially desirable hardness and other properties for swords .
Look up Wikipedia for "Differential heat treatment"
-
24th Mar 2018, 12:52 PM #21Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Gratuitous self promotion here, thanks to BobL for providing a segue. Cherry Red case hardening powder is still available and also the PBC anti-scaling compound. I usually have it going around on eBay but its a little cheaper if you contact me directly as I'm not up for eBay and PayPal fees.
Similar Threads
-
What would be the best method to fix this?
By Zumanity in forum WELDINGReplies: 10Last Post: 15th May 2014, 09:02 AM -
HIGH TENSILE BOLTS Vs MILD BOLTS.
By chambezio in forum METALWORK GENERALReplies: 13Last Post: 3rd Jan 2014, 08:25 PM -
Honing method
By morrisman in forum METALWORK GENERALReplies: 4Last Post: 14th Aug 2013, 10:02 AM -
Making Dickson style quick change tool post holders (picture heavy)
By Dave J in forum METALWORK GENERALReplies: 40Last Post: 9th Apr 2013, 11:15 PM