Aldi LED BBQ light
From time to time, like most on here I suspect, I need to alter the head of a hex head bolt or cap screw. The easiest method I've found of holding the bolt is to grab it by the threads in an ER collet, it doesn't damage the threads and there is no slippage.
In the photos you see a round ER32 collet block in the 3 jaw chuck, and I'm reducing the head of a stainless steel 3/8" countersunk cap screw.
IMG_2984.jpg
IMG_2985.jpg
-
13th Oct 2019, 09:11 PM #2Intermediate Member
- Join Date
- May 2019
- Location
- Tucson, Arizona, USA
- Posts
- 46
I have grabbed it with a nice 3 jaw chuck and it worked fine for me. You method looks more precise.
David
-
13th Oct 2019, 09:35 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
I think it depends on the chuck (and the thread). My main 3 jaw has aggressive serrations on it so that half the time the screw turns in it like a nut.
Michael
-
14th Oct 2019, 02:06 AM #4
Hi Guys,
A trick I often use is to put the screw in a split die and grip the die in the chuck. I used the same method to drill oil holes in M6 CSK hex screws recently.Best Regards:
Baron J.
-
14th Oct 2019, 10:03 AM #5Golden Member
- Join Date
- Mar 2009
- Location
- Melbourne
- Age
- 54
- Posts
- 825
Another quick and dirty method is to cut a matching nut along it's length, screw this onto the bolt you need to turn and clamp onto the nut in the three jaw. The slit allows the nut to act a bit like a collet. When you're done, chuck the nut in a box for next time and you end up with a bit of a collection.
Cheers,
Greg.
Similar Threads
-
Aldi LED BBQ light
By bob ward in forum TIPS, TRICKS & HOW TO'SReplies: 1Last Post: 21st Oct 2019, 09:41 AM -
Tools at Aldi Sat 28 May
By neksmerj in forum METALWORK GENERALReplies: 3Last Post: 26th May 2016, 01:49 PM -
Aldi Welder
By Twisted Tenon in forum METALWORK GENERALReplies: 12Last Post: 4th Oct 2011, 08:16 PM -
Aldi Sale
By Blu_Rock in forum METALWORK GENERALReplies: 11Last Post: 26th May 2008, 09:43 AM