Needs Pictures: 0
Results 1 to 10 of 10
Thread: making an ulu knife
-
6th May 2021, 08:02 PM #1human termite
- Join Date
- Jul 2007
- Location
- sandstone point queensland
- Age
- 69
- Posts
- 182
making an ulu knife
started making this Alaskan ulu knife today from an old saw blade, all was going well except the sanding belt caught on the edge and threw the knife back at me , cut an artery in my wrist and a large cut longways down my thumb. (warning gore alert)......bob
-
7th May 2021, 10:35 AM #2Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Nasty. Thanks for the warning though. I hope there's no permanent damage and you get back into the workshop soon.
What type of belt sander do you have?Chris
-
7th May 2021, 05:30 PM #3
Hi Bob, Guys,
I agree with Chris, very nasty !
It just shows how quickly something can turn on you and cause injury, I hope that it heals rapidly.Best Regards:
Baron J.
-
9th May 2021, 02:37 PM #4Golden Member
- Join Date
- Apr 2018
- Location
- Drouin Vic
- Posts
- 634
'This blade will cut'.
-
9th May 2021, 03:19 PM #5Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
11th May 2021, 08:51 AM #6Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Ouch!
I have had similar things happen with smaller parts grabbing on a linisher and flipping in my hand. Not with the same consequences though.
Get better soon.
Thanks for the pics!
Sent from my SM-G970F using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
18th May 2021, 11:39 AM #7Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
This thread has been sitting there telling me I have'nt looked at...wish I hadnt now
hope there is no permanent damage.
-
24th May 2021, 02:52 AM #8
The curved shape is best completed by "dragging" the cutting edge.
That is, with the belt moving away from the cutting edge.
I made a leather cutting knife of the same shape as an Ulu and found that out.
No, I did not cut myself, but ruined a belt and a idler wheel.
May you recover quickly, Robyn.
Grahame
-
24th May 2021, 05:08 PM #9China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
That is a good point why is it that those of us who are knife makers grind towards the edge when everything that you have ever been told/learnt tells you it is a accident waiting to happen.
-
24th May 2021, 06:41 PM #10
I believe it has a lot to do with the lap of the belt joint .Some belt joints are not as flush as others are.
The geometry of the blade and its size also play a part.
Also whether or not you are supporting the work on the work surface or holding it freehand against the supporting platen make a difference.
I can tell you its a sphincter tightening experience when the blade bites into that belt joint.
The belt parts and slaps you in the chops,while at the same time the blade whistles past your ear. I was fortunate that I was not injured.
Other blade makers can freehand edge first into the belt but I choose not to.
Grahame
Similar Threads
-
I begin to Knife Making
By NolanF in forum METALWORK PROJECTSReplies: 14Last Post: 3rd Jun 2020, 06:21 AM -
Better knife pics
By Briangoldcoast in forum METALWORK GENERALReplies: 13Last Post: 5th Dec 2014, 02:24 PM -
knife help
By new_guy90 in forum METALWORK GENERALReplies: 2Last Post: 27th Apr 2009, 01:49 PM -
Cuttting 6mm mild steel for knife making
By safadao in forum METALWORK GENERALReplies: 10Last Post: 25th Apr 2007, 06:14 PM -
Bog Oak Knife
By buzzy bee in forum METALWORK GENERALReplies: 4Last Post: 3rd Feb 2007, 09:15 PM