    I dabbled in knife making several years ago, turned out a few knives that I was happy with but have not had time to take this up since. I sent a couple of blades to Hills Heat Treating in Bayswater, they were very helpful, reasonably priced and happy to deal with a hobby knife maker- I got the impression they did this a lot.
    A project that I have on the slowburner at present is a bunch of custom archery broadheads. I've ordered some RWL34 stainless for the blades as I was very happy with this stuff in a couple of my knives. I looked up Hills heat treatment with a view to sending the finished blades to them for hardening but it appears they have gone out of business. There appear to be several businesses around offering heat treatment but their websites give the impression that they are focussed on heavy industry. Does anyone know a mob that offer heat treatment and are happy to deal with the little bloke? I don't do enough of this to even contemplate getting a kiln etc myself.

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Now that Hills are no more I use this mob, although they are S.A. Tooling and General Heat Treatment - Home - Adelaide, South Australia

  3. #3
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Thanks for that China, I'll give them a call when i get close to having something to treat. Being interstate isn't an issue, I would have mailed the stuff to Hills anyway.

  4. #4
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Hi Pete, Just a thought in a recent edition of MEW there's an article on making a kiln over several issues.
    Kryn
    To grow old is mandatory, growing up is optional.

  5. #5
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Quote Originally Posted by KBs PensNmore View Post
    Hi Pete, Just a thought in a recent edition of MEW there's an article on making a kiln over several issues.
    Kryn
    I don't have time for the projects I already have going!

  6. #6
    Join Date
    Apr 2009
    Location
    Kingswood
    Posts
    930

    Default

    I took a mate to R&J Heat Treatment in Seton Rd Mooremank (next to Liverpool NSW) recently to pick up a couple of hobby pieces for a small cash payment.
    Chatted quickly at the counter, they seemed very approachable.
    Small industrial single fronted site, 3 guys (near knock-off time), looked good (for a heat-treatment plant) with pallets and bins of goods waiting processing/pick-up, and they have got a good web page.
    My mate swears by them.
    John

  7. #7
    Join Date
    Apr 2018
    Location
    Drouin Vic
    Posts
    634

    Default

    Thanks John, I'll have a look at their website. Nice to know there are still some companies that have not outgrown their customers.

Similar Threads

  1. Regulator / fittings for gas weed burner(for heat treating)
    By StrayAlien in forum METALWORK GENERAL
    Replies: 8
    Last Post: 17th Jan 2017, 07:20 AM
  2. Replies: 7
    Last Post: 15th Aug 2015, 09:43 PM
  3. Replies: 1
    Last Post: 14th May 2013, 08:18 PM
  4. Trouble Heat Treating O1 at Home Consistently
    By thumbsucker in forum METALWORK GENERAL
    Replies: 13
    Last Post: 9th Oct 2008, 04:26 PM
  5. Heat treating very thin blades
    By derekcohen in forum METALWORK GENERAL