    I found the cause of faint scraping noise coming from my lathe motor, the remains of a mummified mouse,some Ratsak and the nest!
    I also discovered why it tripped the RCD, corroded earth wire poked into one of the phase wires.
    Probably not too bad considering the wiring hasn't been looked at since the 1960s.
    Attached Images Attached Images

  2. #2
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,651

    Default

    I reckon that mouse was trying to tell you something…..

    Steve

  3. #3
    Join Date
    Dec 2020
    Location
    Geraldton Western Australia
    Posts
    132

    Default

    Time for a little TLC, cleaned it all, repacked bearings, new heatshrink and tomorrow I'll replace the wiring between the switchgear and the motor.
    Runs very well considering it's age.
    Attached Images Attached Images

  4. #4
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,444

    Default

    Hi Guys,

    One of the original "Brooks Motors" made in Huddersfield UK !

    I've not seen a "Cub" in maybe 50 years or more ! A good solid motor, very heavy for its power output.

    Im194603BTJ-Brook.jpg Im19371231EE-BrookMotors.jpg

    The graphic at the bottom left on the first page is actually an image of the original pre=war Empress works. They later took over some derelict property on the same street in order to expand the works. Mainly warehousing I believe. Then they added some new production faculties in "Doncaster" which doubled the production ability.
    Best Regards:
    Baron J.

  5. #5
    Join Date
    Dec 2020
    Location
    Geraldton Western Australia
    Posts
    132

    Default

    I also have one on my Servian drill press.
    Attached Images Attached Images

  6. #6
    Join Date
    Dec 2020
    Location
    Geraldton Western Australia
    Posts
    132

    Default

    Not sure that I'd like to be near it if it had the Hi-Low pulley running at top speed!
    Attached Images Attached Images

Similar Threads

  1. Noise Reduction
    By Satwinder Singh in forum METALWORK GENERAL
    Replies: 25
    Last Post: 17th May 2020, 10:27 PM
  2. Motor Noise
    By Anorak Bob in forum ELECTRICALS
    Replies: 5
    Last Post: 31st Oct 2017, 09:58 PM
  3. Bearing noise
    By ratters in forum THE HERCUS AREA
    Replies: 10
    Last Post: 13th Feb 2015, 08:19 PM
  4. my noise maker
    By eskimo in forum GUNSMITHING
    Replies: 34
    Last Post: 21st Apr 2014, 11:15 AM
  5. Noise from MH 48 mill
    By Ben Dono in forum METALWORK GENERAL
    Replies: 33
    Last Post: 11th Feb 2012, 05:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •