Sheraton C rebuild
Well, here's an idea of progress to date. See earlier posts for 'as before' pictures.
1) Original state of the headstock shown below as removed from the machine; full of mud wasp debris + surface corrosion. Was semi-seized because it had sat unused for so long.
Headstock before rework @ 40%.jpg
2) After a bit of work...
The thrust bearing was the only part replaced. ($20). The shaft bearings were in pretty good condition considering... was able to use the previous shims.
Headstock @ 40%.jpg
3) The general rebuild thus far. How to keep brain & body usefully engaged over the past few months of 'interesting times'.
Rebuild progress 3 @ 40%.jpg
Starting soon on the carriage & step-down gears at l/h end.
Similar Threads
-
Help with jointer rebuild
By kenny_10 in forum METALWORK GENERALReplies: 12Last Post: 17th Jun 2020, 08:25 AM -
Hercus +rebuild with DRO
By NickMortimer in forum THE HERCUS AREAReplies: 8Last Post: 17th Jun 2016, 09:14 AM -
ARM Rebuild Questions
By rickw72 in forum THE HERCUS AREAReplies: 4Last Post: 17th Aug 2012, 12:22 PM -
Trailer rebuild
By artme in forum TRAILERS & OTHER FABRICATED STUFFReplies: 3Last Post: 29th Jan 2012, 11:15 PM -
Hercus rebuild
By Big Shed in forum THE HERCUS AREAReplies: 1Last Post: 10th Sep 2009, 01:56 PM