High performance grinding wheel
https://www.youtube.com/watch?v=0BoWvFL_80E
A bit on HSS tools and a new grinding wheel with a difference.
-
11th Dec 2022, 05:45 PM #2
Grade
What is the grit size and grade of your wheel . Thanks
-
14th Dec 2022, 09:49 AM #3Senior Member
- Join Date
- Nov 2019
- Location
- Brisbane
- Age
- 69
- Posts
- 452
grinding wheel
Hi Morrisman.
The wheel is a 60 grit Norton high performance. It grinds fast and cool but under the light once turned off the edge showed some wear after the first cutter. A few months will be needed for me to get any idea of life but the usage confirms the old wheel was crap.
Next year i hope to start using CBN wheels.
All the best.
BC
Similar Threads
-
Grinding wheel help
By kenny_10 in forum METALWORK GENERALReplies: 3Last Post: 24th Nov 2022, 08:30 PM -
Grinding wheel
By sossity in forum METALWORK GENERALReplies: 38Last Post: 14th Feb 2017, 06:04 PM -
Grinding Wheel
By Oldneweng in forum METALWORK GENERALReplies: 18Last Post: 15th Jan 2017, 06:07 PM -
Which Grinding Wheel For Grinding Tungsten Electrodes
By Metal Head in forum WELDINGReplies: 14Last Post: 8th Aug 2009, 02:23 PM -
Lap grinding wheel
By ROB NZ in forum METALWORK GENERALReplies: 6Last Post: 20th Jan 2008, 06:42 AM