Making T-nuts for the rotary table
The rotary table has T-slots suitable for M6 T-nuts.
I make 9 T-nuts out of Sverker 21 tool steel.
I also present how to heat treat this particular tool steel.
In this video I am using:
- Schaublin SV-51 (1955) Milling machie
The video is here