Hi
I bought a bench grinder from a flea market couple years ago.
It was little bad condition, and i usually doesn't even use rough wheels for grinding.
I had more use for a finishing machine, so i made this simple mod to it. Big wheel on the right side, is scotch brite polishing wheel.
FB_IMG_1636106251591.jpg
Originally it had been similar than this:
FB_IMG_1636106247066.jpg
Picture is from the internet, mine was missing some parts.
Video about the process:
-
12th Nov 2021, 10:02 AM #2Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
A 5mm hole for a ⅜" tap?
Chris
-
12th Nov 2021, 12:47 PM #3Senior Member
- Join Date
- Apr 2019
- Location
- Finland
- Age
- 46
- Posts
- 117
Whoops. Actual thread size in chuck is 1/4-20. I allways mix those. Specially easily when video editing is made week after actual making process.
Most likely reason was, that i needed to make a new thread to pipe, and searched3/8" - 18 NPT taper thread die with google meanwhile video editing software was rendering video clips.
-
12th Nov 2021, 12:59 PM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,182
I squirmed a bit when I saw the tap continually spinning in the drill chuck. That looks like a good way to damage the chuck jaws.
-
12th Nov 2021, 03:06 PM #5Senior Member
- Join Date
- Apr 2019
- Location
- Finland
- Age
- 46
- Posts
- 117
Similar Threads
-
Very simple angle grinder cutting guide
By Tuomas Soikkeli in forum Members VideosReplies: 4Last Post: 21st May 2020, 05:21 PM -
Gmf bench grinder resto
By china eyes in forum METALWORK PROJECTSReplies: 10Last Post: 14th Apr 2019, 08:51 PM -
bench top for a bench grinder
By wodstok in forum METALWORK GENERALReplies: 1Last Post: 24th Jan 2011, 03:04 PM -
WEST AUST Bench Grinder brand new
By beer is good in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 24th May 2010, 05:28 PM -
Which 200 mm bench grinder should I buy ?
By Retromilling in forum METALWORK GENERALReplies: 15Last Post: 16th Oct 2008, 11:31 AM