Anvil restoration. Dalsbruk number 2
Here anvils are somewhat expensive.
Restoring old ones can save you a big penny.
I found old Dalsbruk anvil from yardsale, it was a little bad shape thought. But, after restoring it, i got nice new tool from it to my shop.
Here is the video about process:
https://youtu.be/xrwudL1FPUs
Similar Threads
-
Grinder Anvil
By YBAF in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 4Last Post: 30th Oct 2020, 12:37 PM -
Help with Anvil
By midlife in forum THE SMITHYReplies: 7Last Post: 26th Jul 2013, 09:54 PM -
Anvil on e Bay
By auscab in forum THE SMITHYReplies: 6Last Post: 28th Jan 2013, 10:34 PM -
SOLD: Anvil
By ranga_rod in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 25th Nov 2012, 04:15 PM -
TASMANIA Anvil
By rwatson in forum METALWORK - Machinery, Equipment, MARKETReplies: 1Last Post: 17th Apr 2011, 07:40 PM