Bought a cheap Chinese Digital Micrometer, here's a bit of a review -
Bought a cheap Chinese Digital Micrometer, here's a bit of a review -
-
25th Oct 2020, 06:11 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Used for measuring inside tube.
-
25th Oct 2020, 06:34 PM #3Golden Member
- Join Date
- Sep 2008
- Location
- Riddells Creek, Vic.
- Posts
- 838
The S shaped tool is used to turn the battery compartment cover I think. The ball anvil can be used to measure the wall thickness of tube etc.
-
26th Oct 2020, 09:53 AM #4
-
26th Oct 2020, 01:02 PM #5Golden Member
- Join Date
- Apr 2019
- Location
- Adelaide
- Posts
- 596
Given that any standard is only correct at a given temperature, how much could that 25mm standard grow or shrink depending on the temperature? Is it something that needs to be taken into account? A quick online calculator just showed 10 degree C change making a 0.004mm change to 25mm so I think I answered my own question!
What were the analogue micrometers reading on that same standard?
All up it looks to be a great bit of kit and worth buying. Maybe do another review after using it for a bit.
Nice one.
Similar Threads
-
Chrome Steel Ball Measure with Digital Micrometer
By electrosteam in forum METALWORK GENERALReplies: 14Last Post: 3rd Oct 2019, 09:10 AM -
Review of the $US32.79 Shahe Digital Micrometer
By RayG in forum METALWORK GENERALReplies: 50Last Post: 17th Oct 2015, 01:17 PM -
Chinese Tig Welder review - 5 years on
By 19brendan81 in forum WELDINGReplies: 23Last Post: 26th Aug 2015, 04:39 PM -
This is clever and cheap - digital readout for lathe - 25mm travel
By steamingbill in forum METALWORK GENERALReplies: 12Last Post: 13th Dec 2013, 07:06 PM -
Dud Mitutoyo Digital Micrometer
By 19brendan81 in forum METALWORK GENERALReplies: 7Last Post: 15th Sep 2011, 06:57 PM