Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 5 of 5
Thread: Removing solder from silver
-
3rd Jun 2022, 12:08 PM #1Senior Member
- Join Date
- Apr 2018
- Location
- Perth
- Posts
- 168
Removing solder from silver
Not really jewellery but I have a old table lamp that is my fathers. It was made many years ago by soldering a copper pipe for the lamp support onto the back of a silver figurine.
I want to remove the pipe and try to restore the silver figurine so am wondering how would be the best way. I was thinking of using my weller iron and a solder sucker to remove the majority but Im sure that will leave traces on the silver.
.20220603_085715.jpg20220603_085637.jpg
-
3rd Jun 2022, 12:39 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
I think solder has a greater affinity for raw copper than sliver so maybe try some of that solder wicking copper braid stuff?
-
3rd Jun 2022, 04:35 PM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Paint around the edge of the solder line with yellow ochre apply fairly heavy or Liquid paper, this will stop the solder flowing further onto the Silver, then as above try solder wick, I do not think this will remove all the solder you will be left with a film that you will need to be removed mechanically. I would use a torch but I have been working with Silver for many years, you may struggle with the weller, if you go with a torch be aware that Silver has low melting point.
-
3rd Jun 2022, 08:52 PM #4Senior Member
- Join Date
- Apr 2018
- Location
- Perth
- Posts
- 168
Thanks Bob and China,
Thinking silver should be harder than solder so could I possibly buff away the solder ?
-
8th Jun 2022, 04:57 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
If you go carefully yes.
Similar Threads
-
SIlver Solder -Suppliers - High silver content
By steamingbill in forum METALWORK GENERALReplies: 25Last Post: 15th Mar 2019, 05:15 PM -
WTB ADL Silver solder rod
By GWH74 in forum WANTED TO BUYReplies: 0Last Post: 28th Apr 2016, 08:19 AM -
245 Silver solder
By fxst in forum METALWORK GENERALReplies: 2Last Post: 16th Oct 2012, 12:22 AM -
source of silver solder other than BOC?
By desbromilow in forum METALWORK GENERALReplies: 6Last Post: 30th Aug 2012, 11:30 AM -
Silver Solder Pt 2 How to
By Grahame Collins in forum METALWORK GENERALReplies: 0Last Post: 11th Jan 2007, 10:51 AM