    Here is Pic of the finished item, posted here as it is a jewellery item

    Mill 1.jpg

  2. #2
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    5,107

    Default

    Hi Bob, Guys,

    Michael has done a superb job . You must be quite proud of it.

    Just don't get a hernia lifting that machine ! It looks like at least 100Kg.
    Best Regards:
    Baron J.

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,420

    Default

    Yes he has, and all credit to him, no I won't be lifting it is staying right were it is ( it is on wheels now ) it weighs 77kilos.
    The less than perfect paint job is my contribution.

  4. #4
    Join Date
    Jun 2012
    Location
    ex Perth, now Mittagong
    Posts
    92

    Default

    My daughter is into jewellery and has a rolling mill and I have been thinking of motorising it. Could you tell me what the motor and gearbox unit is on yours? It looks to be what I am envisaging.

    Peter

  5. #5
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,420

    Default

    Peter I will take a pic of the label tomorrow, the label on the gearbox is a bit hard to access now it is on the bottom of the unit, I am pretty sure the label on the motor label has the all the same info
    it is a 3ph SEW Euro-drive, they don't come cheap I was fortunate that my mate had one from a job that never happened so I got it for nearly half price.
    Although I have 3ph it runs from a VFD as it is simple convenient way to control speed etc while still maintaining torque.

  6. #6
    Join Date
    Jun 2012
    Location
    ex Perth, now Mittagong
    Posts
    92

    Default

    China, Looking forward to any info you can glean.

    Peter

  7. #7
    Join Date
    Dec 2007
    Location
    Sydney
    Posts
    259

    Default

    I picked up a rolling mill for my daughter years ago as she was doing work experience with a friend of my wife who is a jeweller. She seemed a bit interested at the time?
    Anyhow it sat in the shed unused for years, the cast legs went to a mate for his Ewheel.
    My son who is a sparky started scoring large left over cable.
    We made a basic stripper with a piece of square tube and a hard screw.
    Pulling the cable thru that was very hard work, but he got $800 plus for scrap.
    He then gets a heap more and asks about a stripper.
    He bought a hard wheel online and I modded the rolling mill in the old Macson.
    Cut the lower roller into steps and cut teeth in them with an angle grinder.
    Works well, $2000 last lot at the scrapyard.
    If he gets more wed better motorise it.
    H.
    Attached Images Attached Images
    Jimcracks for the rich and/or wealthy. (aka GKB '88)

  8. #8
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,420

    Default

    Looks like it may be an old Cavallin

  9. #9
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,420

    Default

    Peter here is a pic of the id plate

    P1010457.jpg

  10. #10
    Join Date
    Jun 2012
    Location
    ex Perth, now Mittagong
    Posts
    92

    Default

    Thanks for that China, I know what to look for now.

    Peter

Similar Threads

  1. Rolling stand
    By Michael G in forum METALWORK PROJECTS
    Replies: 11
    Last Post: 9th May 2021, 04:18 PM
  2. Plate rolling
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 13
    Last Post: 14th Dec 2018, 01:52 AM
  3. Rolling rings from 8mm rod
    By Scally in forum METALWORK GENERAL
    Replies: 13
    Last Post: 1st Jan 2017, 08:13 PM
  4. Rolling copper
    By denncarm in forum METALWORK GENERAL
    Replies: 5
    Last Post: 27th Oct 2013, 05:15 PM
  5. rolling metal tubes
    By piobuilleann in forum METALWORK GENERAL
    Replies: 2
    Last Post: 29th Jun 2007, 05:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •