Thanks: 0
Needs Pictures: 0
Results 1 to 10 of 10
Thread: Rolling Mill
-
8th May 2021, 01:28 AM #1China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Rolling Mill
Here is Pic of the finished item, posted here as it is a jewellery item
Mill 1.jpg
-
8th May 2021, 07:31 PM #2
Hi Bob, Guys,
Michael has done a superb job . You must be quite proud of it.
Just don't get a hernia lifting that machine ! It looks like at least 100Kg.Best Regards:
Baron J.
-
9th May 2021, 01:25 AM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Yes he has, and all credit to him, no I won't be lifting it is staying right were it is ( it is on wheels now ) it weighs 77kilos.
The less than perfect paint job is my contribution.
-
9th May 2021, 09:19 PM #4Senior Member
- Join Date
- Jun 2012
- Location
- ex Perth, now Mittagong
- Posts
- 105
My daughter is into jewellery and has a rolling mill and I have been thinking of motorising it. Could you tell me what the motor and gearbox unit is on yours? It looks to be what I am envisaging.
Peter
-
9th May 2021, 10:07 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Peter I will take a pic of the label tomorrow, the label on the gearbox is a bit hard to access now it is on the bottom of the unit, I am pretty sure the label on the motor label has the all the same info
it is a 3ph SEW Euro-drive, they don't come cheap I was fortunate that my mate had one from a job that never happened so I got it for nearly half price.
Although I have 3ph it runs from a VFD as it is simple convenient way to control speed etc while still maintaining torque.
-
10th May 2021, 06:44 PM #6Senior Member
- Join Date
- Jun 2012
- Location
- ex Perth, now Mittagong
- Posts
- 105
China, Looking forward to any info you can glean.
Peter
-
11th May 2021, 09:44 AM #7
I picked up a rolling mill for my daughter years ago as she was doing work experience with a friend of my wife who is a jeweller. She seemed a bit interested at the time?
Anyhow it sat in the shed unused for years, the cast legs went to a mate for his Ewheel.
My son who is a sparky started scoring large left over cable.
We made a basic stripper with a piece of square tube and a hard screw.
Pulling the cable thru that was very hard work, but he got $800 plus for scrap.
He then gets a heap more and asks about a stripper.
He bought a hard wheel online and I modded the rolling mill in the old Macson.
Cut the lower roller into steps and cut teeth in them with an angle grinder.
Works well, $2000 last lot at the scrapyard.
If he gets more we’d better motorise it.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
11th May 2021, 03:14 PM #8China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Looks like it may be an old Cavallin
-
11th May 2021, 05:13 PM #9China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,656
Peter here is a pic of the id plate
P1010457.jpg
-
11th May 2021, 07:02 PM #10Senior Member
- Join Date
- Jun 2012
- Location
- ex Perth, now Mittagong
- Posts
- 105
Thanks for that China, I know what to look for now.
Peter
Similar Threads
-
Rolling stand
By Michael G in forum METALWORK PROJECTSReplies: 11Last Post: 9th May 2021, 04:18 PM -
Plate rolling
By KBs PensNmore in forum METALWORK GENERALReplies: 13Last Post: 14th Dec 2018, 01:52 AM -
Rolling rings from 8mm rod
By Scally in forum METALWORK GENERALReplies: 13Last Post: 1st Jan 2017, 08:13 PM -
Rolling copper
By denncarm in forum METALWORK GENERALReplies: 5Last Post: 27th Oct 2013, 05:15 PM -
rolling metal tubes
By piobuilleann in forum METALWORK GENERALReplies: 2Last Post: 29th Jun 2007, 05:22 PM