G'day forumites..
I have some sheet titanium with which I thought I'd try making a pendant. Any tips? I found I can cut it ok with a hacksaw, and a reasonable polish starting with a cheap diamond stone to 600 grit then some 600 wet and dry followed by Tripoli on a buff. Still some scratche though and a few pits on the back.
I also tried heat colour with a little gas burner. Certainly got colour but very subtle. Would ox-acetylene be better? Does anodising give brighter colour?
-
3rd May 2020, 09:52 PM #2Senior Member
- Join Date
- Feb 2012
- Location
- Tamworth, NSW
- Posts
- 202
Do you have any idea what grade of Ti you have? I’ve only used 6AL4v (grade 5) but with this heat colours are quite bright and it anodises very well. There are quite a few online tutorials with anodising - you will want a decent DC power source up to around 120v for all colours. The colours tend to repeat but you tend to get better lasting colour using the higher voltages. I guess because the surface oxide layer you form is thicker.
for multiple colours anodising is fun. If you lay down the highest voltage colour first (mask off the other areas with nail polish or remove some colour via sand blasting etc) you can then continue to add other colours without changing your high voltage colour.
-
3rd May 2020, 10:09 PM #3Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
Absolutely no idea... An auction find, along with a sheet of brass and copper..
Have to dig through the junk box(es) for the makings of a variable supply..
-
3rd May 2020, 10:26 PM #4Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,075
Ti-6-4 is the most commonly used titanium alloy by far, so chances are it's either that or pure titanium
-
6th May 2020, 08:35 PM #5Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
The anodising process is so quick, you can just use 9V batteries connected in series to get the desired voltage (it's almost instant). Of course that only gives you 9V increments. I suppose you could also place a variable power supply in series with the batteries to fine tune the voltage.
Chris
-
23rd Nov 2020, 12:55 PM #6
Titanium colour
I've used titanium inlays for guitars, and my Brit' bro' has used it a lot in his jewellery.
I found that it polished beautifully, taking it to 1200 before putting it on the wheel.
I used Mapp gas - got beautiful rainbow colour, but (with my titanium anyway) I had to seal it pretty soon after to hold the colour, otherwise it just goes dull and grey.
(I used 2K Clear auto finish, It's held it's colour still, after at least 12 years).
-
24th Nov 2020, 08:20 PM #7Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Similar Threads
-
Finishing titanium?
By jhovel in forum METALWORK GENERALReplies: 27Last Post: 23rd Nov 2020, 10:18 PM -
Titanium First Impressions
By jack620 in forum METALWORK GENERALReplies: 12Last Post: 23rd Sep 2018, 11:27 PM -
3D printed Titanium Horseshoes
By BobL in forum METALWORK GENERALReplies: 16Last Post: 19th Oct 2013, 01:38 PM -
Milling Titanium
By glock40sw in forum METALWORK GENERALReplies: 1Last Post: 30th Aug 2007, 07:42 PM -
Titanium
By Chris Parks in forum METALWORK GENERALReplies: 8Last Post: 7th Jan 2007, 10:39 PM