Results 1 to 7 of 7

Thread: An axe to grind

  1. #1
    Join Date
    Jun 2012
    Location
    melbourne
    Posts
    341

    Default An axe to grind

    I wasn't sure if I should bother posting this because I know a lot of you think this sort of thing is pointless as it has no purpose. Think of it as an apprentice piece, because I am just learning.

    I asked PDW for advice regarding what I'd need to get a fine finish on stainless steel. its quite tricky to get a clear optical finish on stainless steel. I didn't know if a small mill would be good enough but he helped me pick out a kondia powermill which I stripped and rebuilt. Machtool rebuilt the quill because i can't work to the precision he does. He also does his own thing regarding technique, which people all over the world argue with him about. Another guy with mad skills. I think the results speak for themselves, as to how fine a finish a bigger mill can give . I find its so time consuming to polish stainless steel, but the mill gives a finish with marks that i think must be sub micron, going by how easy it is to polish. My chinese 300x 1000 lathe gives a nice looking finish but when you try to polish it, its just not flat the same way the mill finish is. I had to spend loads of time polishing the lathe finish and that makes it really difficult to keep a flat surface flat. If you rely on polishing mops, you won't get a dead flat surface.

    This guy https://www.youtube.com/channel/UCwo...nIjS2MA/videos is amazing, but he uses smaller hobby machines. I think the finish he gets off is lathe and mill look really poor, but his skill makes up for it when he finishes parts by hand. In this one though, even his skills don't make up for the poor quality machining, and this is just working in brass and aluminium. https://www.youtube.com/watch?v=a3V42KwLTeE its something people argue over quite often, but for me its been worth getting a second hand professional mill.
    Attachment 383913Attachment 383912
    It was something I always wondered, if you really need to get industrial quality machines for home stuff. I was glad I asked PDW's advice.
    Attached Images Attached Images

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    Not pointless to me, thanks for the post, I appreciate fully the work that goes into something like this, and for those who
    think it is pointless they are ones missing out, it is a thing of beauty and skill.

  3. #3
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Well done. A very nice piece of work.

    Michael

  4. #4
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Very nice work,
    I have seen a welded axe and stump before but never one taken to that level of finish.

    It is only pointless to those that can not appreciate the skill and patience needed to achieve that high level of work.

    Grahame

  5. #5
    Join Date
    Jun 2012
    Location
    melbourne
    Posts
    341

    Default

    Thanks for the kind comments guys, that's made my day. I wasn't sure at all how an arty farty thing would go down in such an egnineery orientated forum.

    There's actually a bit more to it. My father-in-law was a welder in the clyde shipyards in the 50/60's. He made one of these and it was amazing quality, especially because he used hand tools and said he built it up one drip at a time (obviously not with a 600 amp stick welder). I suspect a lot of welders made something like this in their spare time back then. My wife grew up with it around and never realised he had actually made it, she thought it was something bought. We left glasgow 25 years ago and never saw him again. Family's being what they are when it comes to money, we got nothing at all from his moveable estate despite her being sole heir. Think Donald trump as an executor. My wife would have loved his model, because he made it. Anyway, this is a present for her xmas. Its as close as i can remember, in fact I am very pleased how close. To this day i don't know how he welded the axe onto the stump. I did mine in a kind of obvious way, but thats not what he did. His axe just grew out the SS and I can only imagine he did as he said, and dripped it on. How he managed to then file it back into shape and keep such a flat top with such a fine finish is beyond me. Stainless is very slow to work with by hand.

  6. #6
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    As I said earlier, I first saw one years ago.It was featured in the Lincoln periodic booklet for the trade that came out a couple of times a year.

    I marveled at the bark pattern on the stump created by careful arc placement. I recall it had a matchbox beside it for scale.

    I thought it was great, but yours is better by a country mile.

    Arc art is what I call it.

    First class!

    Grahame

  7. #7
    Join Date
    Nov 2010
    Location
    Frankston south
    Posts
    102

    Default

    Beautiful

Similar Threads

  1. How to grind this threading tool?
    By jack620 in forum METALWORK GENERAL
    Replies: 12
    Last Post: 17th Apr 2019, 09:10 AM
  2. Replies: 11
    Last Post: 16th Nov 2018, 12:50 AM
  3. Lathe tool holder too thick - can I grind it down?
    By jabell in forum METALWORK GENERAL
    Replies: 8
    Last Post: 24th Nov 2014, 09:14 PM
  4. Can someone grind a MT1 taper on a threaded rod for me.
    By Sturdee in forum METALWORK GENERAL
    Replies: 7
    Last Post: 27th Apr 2013, 09:49 AM
  5. need somewhere to surface grind some pbar stock??
    By holmsy2000 in forum METALWORK GENERAL