Hi guys, I started to make porcelain jewellery. Now I have a task to attach beautifully a porcelain piece to copper or golden base. I have this way in mind:
1. Object: Firing a porcelain piece with a loop of a kanthal wire inside;
2. Base: Taking the copper or gold base;
3. Junction: Melting a small piece of gold into a drop on the copper / gold base and dipping the loop of a kanthal wire in it; according to my plan it should cool down and stay like that.
As soon as I am zero in this topic: tell me where I fail?
edit: ok now I've read that copper is toxic?
-
21st Dec 2017, 01:11 PM #2
Hi tts_happen
Welcome to the Metalwork forums.
The following was a cut and paste from Wikipedia
In solid form and as finished objects, beryllium copper presents no known health hazard.[2] However, inhalation of dust, mist, or fume containing beryllium can cause the serious lung condition, chronic beryllium disease. That disease affects primarily the lungs, restricting the exchange of oxygen between the lungs and the bloodstream.
The International Agency for Research on Cancer (IARC) lists beryllium as a Group 1 Human Carcinogen. The National Toxicology Program (NTP) also lists beryllium as a carcinogen.
As far a the rest of your enquiry is concerned I will leave that to be answered by our members in the jewellery subforum.
Grahame
-
21st Dec 2017, 03:21 PM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Hi_tss happen
I think you may find it is a case of trial and error, using plain gold as a solder I do not think you will be successful the use of a flux + gold solder will be required to make a solid joint.
To understand the soldering process have a look here (3 video's) https://www.youtube.com/watch?v=J95soMXxhNc , as said before I using some scrap and trying out the process and seeing what occurs will be the best
method.
Similar Threads
-
Acid resistant brass screws
By georgedgerton in forum METALWORK GENERALReplies: 2Last Post: 14th Nov 2015, 05:02 PM -
Cheap gold plating?
By wsal in forum METALWORK GENERALReplies: 10Last Post: 26th Jan 2015, 07:27 AM -
Help to pick up item near Gold Coast
By kwijibo99 in forum METALWORK GENERALReplies: 3Last Post: 30th Mar 2014, 09:57 PM -
copper wire, flux removal
By Kym in forum METALWORK GENERALReplies: 6Last Post: 13th Nov 2008, 03:04 PM