    Default Titanium spectacles repair

    Not quite jewellery, but close.

    I managed to roll over in bed and remove the nose piece from my titanium frame specs.
    Optician tells me they send to qld for soldering, cost 65, but I only paid half that for the frames.
    Is a home repair feasible?.
    I have tig, or soft solder. Or I could glue - super glue or a uv setting resin.
    Photo attached, although hard for you to see cos I've wrapped it up with wire so I can see...
    Probably a neat wire wrap and a touch of soft solder would do the trick. At least while I get new frames.
    I wasn't due for new specs for 12 months at least...

    -russ

  2. #2
    Join Date
    Nov 2010
    Location
    Gippsland Victoria
    Posts
    733

    Default

    https://www.youtube.com/watch?v=xTsfwL61CR8

    Very first example is leg of glasses rather than nose but principle seems the same. Cheap enough to buy it and have a go, I got some at ALdi for $10 a while ago.

    Is it possible to make a jig or a cradle of some sort to ensure no twist when you glue it ? Don't want the lenses pointing in different directions.

    You could leave the wire on, get the lenses positioned right then simply use the bondic to stiffen and cement the wire to the frame - can be buiolt up in multiple passes. Would possibly look ugly but be quite functional ?

    Bill
    Last edited by steamingbill; 3rd Nov 2017 at 06:16 PM. Reason: added jig, added stiffening idea

  3. #3
    Join Date
    Oct 2015
    Location
    melbourne
    Posts
    473

    Default

    Actually I do have that glue, or a copy of it..
    Fortunately the bridge between lenses is intact, this is just the nose piece. But I suspect the joint will be fragile so I do need to align it carefully.

    I wonder if I can find gold (plated) wire. If I can wrap it neatly (if) it might almost look like a feature.. Titanium spectacles repair

    I do wonder if soft solder would take. Gold plating on electronic components takes solder well.

    -russ

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Take it to a manufacturing jeweller most these days have Orion welders that can do the job, as for price you may have to haggle

Similar Threads

  1. Finishing titanium?
    By jhovel in forum METALWORK GENERAL
    Replies: 27
    Last Post: 23rd Nov 2020, 10:18 PM
  2. 3D printed Titanium Horseshoes
    By BobL in forum METALWORK GENERAL
    Replies: 16
    Last Post: 19th Oct 2013, 01:38 PM
  3. Perfectly cleaning titanium
    By benupton in forum METALWORK GENERAL
    Replies: 2
    Last Post: 6th Aug 2013, 01:23 PM
  4. Milling Titanium
    By glock40sw in forum METALWORK GENERAL
    Replies: 1
    Last Post: 30th Aug 2007, 07:42 PM
  5. Titanium
    By Chris Parks in forum METALWORK GENERAL
    Replies: 8
    Last Post: 7th Jan 2007, 10:39 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •