motor shaft end float - is 2mm excessive?
Hi all,
I'm giving some love to a Waldown C-0 tool post grinder. The shaft has about 2mm of float - which to me seems a bit excessive. Full extended in one direction the fan rubs every so slightly, and back the other way, something else rubs ever so slightly ... so I've a feeling this isn't how it is supposed to be.
The Waldown parts list for a C-0 doesn't go into the motor parts so I'm not sure if there should be wave washers or shims or whatever. But a teardown by Max Grant here: https://youtu.be/7QoXMNJueDs shows no washers or shims in there so likely not.
All comments and thoughts welcome.
Greg.
-
18th Sep 2020, 09:00 AM #2Member
- Join Date
- Nov 2016
- Location
- Gulfview Heights, Adelaide
- Posts
- 83
It does not sound right to me. Are the bearings original? I am wondering if they are the correct size.
Paul
-
18th Sep 2020, 09:21 AM #3Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks Paul. Not sure if bearings are original, but they are SKF and have 'Australia' on them - so maybe not that recent. They are a 6200 size, and that is the same size shown in the Max Grant rebuild.
If not original, maybe the originals were 1mm each thicker. Not sure if there is such a thing but I'm no expert.
-
18th Sep 2020, 03:56 PM #4Member
- Join Date
- Nov 2016
- Location
- Gulfview Heights, Adelaide
- Posts
- 83
I think the bearings are the correct ones. Where is the bearing/shaft loose? On the shaft or the outer bearing radius?
The bearing on the pulley end should be a press fit on the shaft and the housing.
Paul.
-
18th Sep 2020, 03:59 PM #5Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks Paul - bearings are press fit onto shaft. The gap is in the bearing to housing in each end plate. Many motors I pulled apart have wiggle room there for wave washer or two in them to deal with that float.
-
18th Sep 2020, 07:41 PM #6
I'd just add a 2 wave washers.
I bought some 28mm ones recently and they are cheap in a 10 pack.
They have a good wave to them so 1 will do it for 1mm at each end.Using Tapatalk
-
18th Sep 2020, 07:45 PM #7
Hi Greg, Paul,
Greg I think that you may be correct, there should be a wave washer in there. If someone has had it apart it isn't always obvious that there is a washer in the housing, and like me would have put it down on the bench and the washer drops out and ends up on the floor unnoticed.
Putting new ones in would not go amiss !Best Regards:
Baron J.
-
19th Sep 2020, 08:45 AM #8Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
Thanks Baronj, Paul,
That seems to be the case - I reckon I'll just bung em in and see. I'll order some of those.
Then wait a fortnight for delivery!
Thanks again. 👍
Similar Threads
-
motor output shaft sizing
By Harry72 in forum METALWORK GENERALReplies: 11Last Post: 26th Apr 2016, 09:06 AM -
electric motor shaft extension.
By th62 in forum METALWORK GENERALReplies: 3Last Post: 19th May 2014, 12:08 PM -
What machine to sharpen a Float?
By FenceFurniture in forum METALWORK GENERALReplies: 5Last Post: 28th Sep 2012, 04:44 PM -
motor shaft dilemma
By morrisman in forum METALWORK GENERALReplies: 45Last Post: 11th May 2012, 08:26 PM -
Bushing a elec motor shaft.
By Harry72 in forum METALWORK GENERALReplies: 11Last Post: 23rd Oct 2005, 11:41 PM