    I will jump on board about connon motor. I two am another happy customer. I had a few issues about setup and rang them. They were very helpful and steered me in the right direction.

    So back to your original question about if it is worth it. For me I think so. If I am turning a bit of unknown steel i can dial the speed up or down a bit and find a speed where it is happy cutting. It is also great if you finish a cut and want to wind it up to maximum revs for a quick polish.

    When I set mine up I put a three speed pulley on it. The middle speed does 90% of what I need. If for some reason I want super slow or crazy fast I will do a change with the belt.

    If you have the space don't be afraid to go for a slightly bigger motor. That way you will have good power at low speed.

    Steve

  2. #32
    Join Date
    Oct 2019
    Location
    Tasmania
    Age
    53
    Posts
    150

    Default

    Quote Originally Posted by Halifax614 View Post
    Hi Danshell & Baron J. Many thanks for the responses.
    I had a look at Conon's website; very interesting! The 0.55Kw 3 ph.motor that you show & the BD600 VFD to drive it (F1-H100S20007BXO, is that correct??) are a not unreasonable price, bearing Danshell's comment about the certainty of them working together.
    Would you be able to photograph the new motor & belt drive, & VFD main box installation on your SB lathe & post them here?
    Perhaps I should stop further work on the original step-down arrangements until I've weighed this up further?

    Rgds. H614
    Hi Yes that is the model VFD I bought. The website image is different to the actual VFD but the model number is correct.

    It is a little difficult getting photos due to the lathe being against the wall but I tried. I can still move my cone pulley belt around on the lathe to change the configuration but I dont need to. (i really should have the belt on the right hand side, or smaller drive pulley) and the larger pulley that the motor drives has a step up but again I dont change that either now.
    And likewise, the VFD install is just under the bench out of the way, so I took the cover off and got a photo of the massive amount of wires running out of it for you.

    Let me know if that helps.

    IMG_4564.jpg

    IMG_4563.jpg

    IMG_4565.jpg

  3. #33
    Join Date
    May 2018
    Location
    Cairns, Qld.
    Posts
    70

    Default VFD Drive

    Danshell & Reidy 41 - Your comments & photos re: the VFD installation are a huge help.
    I did wonder if you'd done away with the whole step-down pulley arrangement & gone directly from the motor to the main spindle, but I see that's not the case.
    I have today just about finished the main part of the Sheraton rebuild, i.e. the 'lathe' section (Will post a few more photos over in that area soon), so I'm moving on to the 'drive' bit next....

    I did watch about a third of Bob L's Men's Shed video about VFD's etc, but ran out of time the other day. I'll finish it very soon. I'm a Men's Shed member on the opposite corner of the country.

    Thanks very much to all for your assistance.

    H614

  4. #34
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Another thing you might find useful is the "VFDs for Newbies" PDF located in the woodies forum
    https://www.woodworkforums.com/f271/vfds-newbies-232742

    I think you need to be a member to be able to download the document.

  5. #35
    Join Date
    Oct 2019
    Location
    Tasmania
    Age
    53
    Posts
    150

    Default

    Quote Originally Posted by Halifax614 View Post
    I did wonder if you'd done away with the whole step-down pulley arrangement & gone directly from the motor to the main spindle, but I see that's not the case.
    I wanted to keep my lathe as original as I could so I left everything in place. Besides the modern looking VFD hidden under the bench it looks like it belongs in a better era

Page 3 of 3 FirstFirst 123

Similar Threads

  1. Vfd remote switches.
    By eskimo in forum ELECTRICALS
    Replies: 9
    Last Post: 8th Jun 2019, 11:22 AM
  2. Switch Enclosure- Switch Position Identification.
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 17
    Last Post: 19th Jul 2016, 11:00 AM
  3. VFD Remote Cable
    By Oldneweng in forum METALWORK GENERAL
    Replies: 18
    Last Post: 14th May 2014, 07:39 AM
  4. Switch Panel Graphics for Dummies
    By Bryan in forum METALWORK GENERAL
    Replies: 8
    Last Post: 19th Apr 2011, 11:01 PM
  5. VSD Remote Control Panel Questions
    By markjaffa in forum METALWORK GENERAL
    Replies: 28
    Last Post: 20th Apr 2010, 05:15 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •