Opinions on Sharpening Router Bits?
Is it really a viable option, especially for bits with a specific diameter such as 3/4 or 1/2 inch? How can they be sharpened without affecting their diameter?
-
15th Jul 2020, 11:32 PM #2Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,075
Yes it is viable (and very common), yes it affects the diameter, you just change your tool offset to allow for it.
-
16th Jul 2020, 05:46 AM #3
Hi Guys,
You will need a diamond wheel for the carbide !Best Regards:
Baron J.
-
16th Jul 2020, 09:25 AM #4Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,182
Similar Threads
-
Small HS Router Bits
By electrosteam in forum CNC ForumReplies: 6Last Post: 23rd Nov 2017, 11:54 AM -
Router bits
By phaser in forum METALWORK GENERALReplies: 11Last Post: 1st Mar 2017, 11:14 PM -
router bits in lathe to mill aluminium - youtube video
By steamingbill in forum METALWORK GENERALReplies: 3Last Post: 29th Oct 2013, 06:55 PM -
Hand Sharpening Drill Bits
By Grahame Collins in forum METALWORK GENERALReplies: 46Last Post: 25th Jul 2011, 12:29 AM