Results 1 to 14 of 14
  1. #1
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default CNC plasma table anywhere near Central Victoria?

    Do we have any members or their friends with a CNC plasma table willing to do some cutting of 2 or 2.5mm steel sheet?
    I want to cut a pile of 'Kantwist' type clamps (just the sides). If that person wants to part of the collaborative project, I'm happy to ' pay' in suitable steel....

    Cheers
    Joe
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  2. #2
    Join Date
    Sep 2019
    Location
    Nagambie vic
    Posts
    22

    Default

    I’m not sure of anyone personally but there’s a few engineering businesses in Shepparton or Bendigo that probably have one. Or are you trying to do a “mates rates” type of deal? No judgement if you are, it definitely makes things more affordable CNC plasma table anywhere near Central Victoria?

  3. #3
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    Yes I was hoping that someone might want some clamps too and I'll supply the materials....

    Cheers
    Joe
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  4. #4
    Join Date
    Dec 2011
    Location
    Sydney
    Posts
    505

    Default

    Hi Joe,
    A group 'Kant Twist' clamp project sounds interesting.
    What size(s) do you have in mind?
    Cheers,
    Bill

  5. #5
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    I was hoping to make several sizes. 2", 3" an 4"...

    Cheers
    Joe
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  6. #6
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    Just found some instructions on how to make them without using any CNC - or other machine tools at all.....
    That would be an interesting group build:
    https://www.youtube.com/watch?v=6fcKVGtcOdI
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  7. #7
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Smile

    Hi Joe,

    My eyesight is fading with age; but that youtube example certainly looks like crap.

    Some of my scrap pile looks to be better quality material.



    Ken

  8. #8
    Join Date
    Feb 2009
    Location
    moonbi nsw Aus
    Age
    69
    Posts
    364

    Default

    Joe, I don't think you could work as rough as the bloke in the vid. Obviously quality is not a concern of his. It is good for the "concept" though
    Just do it!

    Kind regards Rod

  9. #9
    Join Date
    Nov 2017
    Location
    Geelong, Australia
    Age
    57
    Posts
    2,673

    Default

    FWIW, I've been meaning to make some up for a while, so got off my bum have a couple being laser cut now from 3mm plain steel.
    Its working out at around $3 per plate, so $12 per clamp (includes material). I inquired about per-part costs reducing for a larger order, but it won't reduce as there's no setup cost involved - just cutting and material.

    Steve

  10. #10
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,481

    Default Kant Clamps.

    Hi Guys,

    I did a write up on how I made mine. I've just done a search through my pictures on the forum to find that a number of them relating to this post are now missing !

    https://metalworkforums.com/f65/t200...ht=Kant+clamps

    21-10-2017-001.JPG 01-09-2017-003.jpg

    These are laser cut from 3 mm sheet. Be aware that the edges may be very hard. I took off the sharp bits with my DE grinder.
    Best Regards:
    Baron J.

  11. #11
    Join Date
    May 2005
    Location
    Cockatoo Vic
    Posts
    84

    Default

    Quote Originally Posted by jhovel View Post
    Do we have any members or their friends with a CNC plasma table willing to do some cutting of 2 or 2.5mm steel sheet?
    I want to cut a pile of 'Kantwist' type clamps (just the sides). If that person wants to part of the collaborative project, I'm happy to ' pay' in suitable steel....
    I know this is an old post but thought I might respond anyway.

    These could be done on my CNC plasma.

    I am a hobby user and do not expect profit.

    Cockatoo. East of Melbourne.

  12. #12
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    Hi Greolt.
    Thanks for the offer! What software do you use to drive your plasma?
    Any photos of your setup? I'm actually contemplating building one for myself.... but it is down the list a bit....
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  13. #13
    Join Date
    May 2005
    Location
    Cockatoo Vic
    Posts
    84

    Default

    I posted some pics in this other thread.

    https://metalworkforums.com/f308/t205455-cnc-plasma-play/latest/post1979959#post1979959


    Controller is UCCNC. CAD CAM is Vectric Cut2D

  14. #14
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,105

    Default

    Thanks Greg. Had a look at all your videos and posts.
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

Similar Threads

  1. G'day from Central Coast NSW
    By Vicval01 in forum G'day mate - THE WELCOME WAGON -Introduce yourself
    Replies: 8
    Last Post: 6th May 2020, 11:03 AM
  2. can someone in central victoria (goldfields) lend a hand in emergency?
    By miss_emma_jade in forum METALWORK GENERAL
    Replies: 36
    Last Post: 13th Jun 2015, 12:57 PM
  3. Replies: 37
    Last Post: 20th Nov 2014, 11:43 PM
  4. New member from Central Coast
    By Dono in forum METALWORK GENERAL
    Replies: 12
    Last Post: 1st Jan 2013, 10:31 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •