The mh28 looks almost identical to the G0704. As such, the general conversion scheme should be the same. The specs I found indicate that it is a tad bigger than the G0704 so you will have to adjust dimensions a bit, but stepper sizes and such should work fine.
-
15th Jan 2020, 10:14 PM #17
Hi Guys,
As some may know, I have a BF20L mill. One of the issues with it is that the square cross section column has most of one face removed and dovetails down each side. The head is carried on a bracket that slides in the gap created on one face of the column and is raised and lowered by a screw inside the column. The bracket is not a good fit in that gap and relies upon the dovetails guiding the head to keep everything square.
The problem that arises is the locks for the head bear on the gibb strip on the right hand side looking from the front of the mill. When the locks are tightened the square column casting compresses and twists the head slightly out of tram. This leaves the column very slightly curved and the dovetails curve with it. This causes the head tram to vary with hight up the column. A side effect of this is the column will twist under a too heavy a cut, this can be seen as the head shaking from side to side.
The real cure for this is to make the head bracket a good fit in the gap and stop the column from flexing. However it would also make the head harder to move since it would be tighter in the middle and loose at the top and bottom.
I don't see any answer for this problem without a major redesign of the column and head hight adjustment mechanism.Best Regards:
Baron J.
Similar Threads
-
Milling macine
By woodfast in forum METALWORK GENERALReplies: 2Last Post: 9th Apr 2012, 07:57 PM -
which milling arbor
By azzrock in forum METALWORK GENERALReplies: 53Last Post: 15th May 2011, 12:54 PM -
A little help with my first milling machine
By festy_ in forum METALWORK GENERALReplies: 36Last Post: 13th Apr 2011, 11:34 PM -
Milling job
By addy paddy in forum METALWORK GENERALReplies: 1Last Post: 22nd Oct 2009, 10:25 PM -
which milling M/c
By Dusty Wheels in forum METALWORK GENERALReplies: 11Last Post: 26th Mar 2007, 09:19 AM