Does anyone have experience with ABS sheet I know it can be formed using heat, can it just be slumped over a mould or does it need to to pressed
-
6th Jan 2022, 06:49 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
It will sort of slump, but won't form detail without something forcing it. Also, lots of these plastics will try to shrink back to a less stressed form when heated, so you may have a problem with it wrinkling and changing size. Remember those chip packets you used to put in the oven to get minitures? Same sort of thing applies.
Michael
-
6th Jan 2022, 08:59 AM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
What is it you are trying to achieve?
Some pics might be useful.
-
6th Jan 2022, 04:05 PM #4China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
I need to make a rifle case I can not find a commercial one that will fit, I can easily make one from timber, however I thought ABS would be much less weight, making a timber form would not be a problem, although heating a sheet large enough to use a die type form would be, If it could be just slumped over a form it would be doable .
Seems like timber may be the best way to go.
-
6th Jan 2022, 04:19 PM #5Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Something like this?
Box2.jpg
No - not rifles, but chainsaw bars
When all 5 slots are occupied its bloody heavy.
Boxopen.jpg
-
6th Jan 2022, 05:01 PM #6China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
No I was going to just make a conventional type, however on thinking about it, I like that design, it has several advantages over the normal rifle case configuration, some food for thought.
-
6th Jan 2022, 07:32 PM #7Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Along with "bomb" like looking gas forge (which I have sold), SWMBO reckons the department of homeland security would take a keen interest in me walking around in public with such a box.
-
6th Jan 2022, 08:29 PM #8
-
7th Jan 2022, 04:55 AM #9China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Yes I could go the vacuum rout, except I don't have a vacuum pump, and heating the sheet would be problematic, I don't really want to spend a few hundred on a set up that I will use once.
-
7th Jan 2022, 07:30 PM #10Most Valued Member
- Join Date
- Mar 2011
- Location
- Southern Flinders Ranges
- Posts
- 1,555
Lay it up in carbon fibre or fibreglass
A box like that is petty simple to make the reverse form for
-
7th Jan 2022, 10:16 PM #11
-
7th Jan 2022, 10:56 PM #12China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Thanks for all the input, time to go back to the drawing board and decide which way to go, I will try and take some pics of the process, when I decide what the process is.