"Not sure were to ask this question, but I have a Otto Benz blowlamp (old)
and have been trying to find what fuel to use. I've tried kero but it doesn't get up
to a proper flame. A lot of info on the net says petrol (gasoline as they say over there)
Now I'm a bit of a coward so want to know if anyone has any knowledge of
these lamps.
I remember as a wee fella (many moons ago) Mum had an iron heated by petrol
so they must have used petrol in some things, and these lamps seem reasonably
common in the USA.
The company of old Otto became Benzomatic.
Would put up a photo if I knew how to get it off the phone.
Any info would be appreciated,
Cheers
Robb41"
ps I'm Robbo37 on the WWF
-
4th Aug 2020, 12:41 PM #2Golden Member
- Join Date
- Mar 2009
- Location
- Melbourne
- Age
- 54
- Posts
- 825
G'day Robb,
I would have thought kero would be fine but another option would be shellite.
Fuel options with these is set by the size of the jet, petrol versions have much smaller jets so you need to be a bit careful or you'll end up with a fireball.
Are you getting the vaporizer tube hot enough before you turn the fuel on?
A tip with these is pre-heat the vaporizer tube with metho rather than kero which avoids the buildup of carbon and keeps them cleaner.
Cheers,
Greg.
-
4th Aug 2020, 02:48 PM #3Novice
- Join Date
- Oct 2018
- Location
- Dandenong
- Posts
- 13
-
5th Aug 2020, 01:44 AM #4Golden Member
- Join Date
- Oct 2008
- Location
- Cairns, Q
- Posts
- 666
Does it have a cup below the vaporiser for metho to burn and preheat the vaporiser? If not it was probably designed to run on Shellite as Greg suggested. Back in the day Shellite was commonly used in petrol irons, petrol pressure lamps and stoves. I was surprised to see that it is still available:
https://www.bunnings.com.au/diggers-...E&gclsrc=aw.ds
Frank.
-
5th Aug 2020, 10:06 AM #5Novice
- Join Date
- Oct 2018
- Location
- Dandenong
- Posts
- 13
-
5th Aug 2020, 04:11 PM #6
I still have a couple of my father's Tilley blowlamps that were in use through my childhood and teen years. Primary fuel was Kerosene, and they have the cup under the vaporiser for preheating. The cup is filled with metho and lit. The metho should burn for a couple of minutes, heating the vaporiser. The kero tank is pressurised before the metho is placed in the cup and lit, and when the metho is about exhausted, the control valve is opened and the kero vapor flows and is ignited by the metho flame, and the control valve is adjusted to suit the task.
Always allow the burner to fully cool before replenishing the kero or metho to relight, there is a danger of explosion if metho meets a hot burner.I used to be an engineer, I'm not an engineer any more, but on the really good days I can remember when I was.
-
5th Aug 2020, 05:21 PM #7Novice
- Join Date
- Oct 2018
- Location
- Dandenong
- Posts
- 13
Thanks, I have a couple of the Sievert kero blowlamps but from what I can glean from the WWW these use petrol.
Someone else said to try Shellite and that is basically petrol before all the additives are put in, same flashpoint etc.
Having worked in the oil industry for quite a few years, I'm pretty wary of the stuff.
Cheers
-
9th Aug 2020, 02:00 PM #8Novice
- Join Date
- Oct 2018
- Location
- Dandenong
- Posts
- 13
Otto Bernz Blowlamp
I bit the bullet and took the lamp outside, put some petrol in (extinguisher at hand) and warmed it up
with metho then slowly brought in the petrol....all good with a nice blue flame.
Can't work out how to attach a video, sorry.
-
11th Aug 2020, 10:31 AM #9Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,255
dad just used kero. He put a small piece of rag in the cup and filled with kero..this got the temperature up to get the kero warm enough so that atomized fully when leaving the jet.
I used Shellite in my camping lanterns and cooker as it burned cleaner
Similar Threads
-
Primus lamp wick feeder pinion
By Steamwhisperer in forum METALWORK PROJECTSReplies: 9Last Post: 8th Jul 2018, 12:21 AM -
CQ6230A work lamp question
By Ron Hall in forum METALWORK GENERALReplies: 3Last Post: 2nd Apr 2014, 06:42 PM -
An attempt at improving a H and F Lamp.
By Anorak Bob in forum METALWORK GENERALReplies: 6Last Post: 11th Jul 2011, 11:01 PM -
H and F Halogen Lamp
By Anorak Bob in forum METALWORK GENERALReplies: 13Last Post: 25th Dec 2010, 09:35 PM -
Project Lamp
By ro4441 in forum METALWORK GENERALReplies: 5Last Post: 6th May 2009, 07:36 PM