    Default Nothing like the smell of sulphurised cutting oil smoke in the morning

    After not using my mill since last Xmas due to a number of reasons, one of which included a dark coloured dog, I was able to get in and do a small job yesterday. Nothing special, in fact so not special I'm not posting pics.
    Just drilling and tapping 10 T nuts.
    I have some nice little clamps that can't use studs any larger than 10mm dia and as I couldn't buy T nuts to fit my mill with 10mm holes, a few months ago I bought some undrilled T nuts.
    On Sat I went and bought some Hi Tensile 10mm threaded bar and yesterday got stuck in on the mill to to the nuts. Job went ok. Set them up in 2 lots of 5. Dropped them upside down into the slot on the table and just lightly clamped the ends to hold them down.
    Even tried out the old tapping head that I have had for about 6 or 7 years but never used. Haven't used one of these since about 1976.
    Didn't realise how much I had missed the smell of hot cutting oil.
    Now my wife is trying to think up some machining projects for me.

    peter

  2. #2
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    "Nothing like the smell of sulphurised cutting oil smoke in the morning"

    I always thought that saying was meant for black powder..lol

  3. #3
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Peter, good to see you back at the mill.

    Do you have a horizontal bandsaw? One project that I've just added to my (long) list to do is a clamping plate for the bandsaw.

    Saw it on here recently I think (on phone so can't grab the link). It's just a flat piece of steel with a grid of threaded holes to allow clamping of pieces of whatever size and at whatever angle you desire. One end has a 45° angle to better support 45° cuts. Much more versatile than the bandsaw vice. You can just clamp the plate in the bandsaw vice, or probably better tap some holes in the saw and bolt it down.

    Your T nuts reminded me of it, because you would use the mill clamping kit with it.

  4. #4
    Join Date
    Aug 2008
    Location
    Charlestown NSW
    Age
    65
    Posts
    1,673

    Default

    Quote Originally Posted by pippin88 View Post
    Peter, good to see you back at the mill.
    Thanks. I dont really have any projects for it atm but its nice to have it set up so I can use it now

    Quote Originally Posted by pippin88 View Post
    Do you have a horizontal bandsaw?
    No. I dont have any room for one here either. Hoping not to have to be cutting much big stuff so will see how I go.

    Quote Originally Posted by pippin88 View Post
    One project that I've just added to my (long) list to do is a clamping plate for the bandsaw.

    Saw it on here recently I think (on phone so can't grab the link). It's just a flat piece of steel with a grid of threaded holes to allow clamping of pieces of whatever size and at whatever angle you desire. One end has a 45° angle to better support 45° cuts. Much more versatile than the bandsaw vice. You can just clamp the plate in the bandsaw vice, or probably better tap some holes in the saw and bolt it down.

    Your T nuts reminded me of it, because you would use the mill clamping kit with it.
    Sounds like an interesting project.
    peter

Similar Threads

  1. Up in smoke
    By neksmerj in forum GENERAL DISCUSSION / OFF TOPIC
    Replies: 38
    Last Post: 5th Oct 2015, 09:15 PM
  2. Free energy, smoke and mirrors or BS?
    By neksmerj in forum METALWORK GENERAL
    Replies: 41
    Last Post: 1st May 2015, 09:14 PM
  3. can you smell smoke?
    By azzrock in forum METALWORK GENERAL
    Replies: 10
    Last Post: 30th Aug 2012, 02:30 AM
  4. Musty box smell
    By Michael G in forum METALWORK GENERAL
    Replies: 35
    Last Post: 4th Jan 2012, 07:31 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •