  1. #46
    Join Date
    Mar 2011
    Location
    Dural NSW
    Age
    82
    Posts
    1,203

    Default Metric Problems

    Quote Originally Posted by Steamwhisperer View Post
    Thanks Ray but you are being too kind.
    This bit shows the repair to the taper pin in the bevel gear that goes on the shaft in the outrigger arm and the vein opening error I made.

    Phil
    Attachment 380454 Attachment 380455 Attachment 380456 Attachment 380457 Attachment 380458 Attachment 380459 Attachment 380460 Attachment 380461 Attachment 380462 Attachment 380463 Attachment 380464 Attachment 380465 Attachment 380467 Attachment 380466
    Phil
    This metric stuff can cause problems at times.
    You have done a great job.
    Bruce

  2. #47
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Phil, I have a collection of imperial pin reamers from 0 up to 5 I think. Would you like me to put one in the post so you can correct this 'grievous error'?

    Michael

    PS - if you calculate the difference in diameter between a 1:48 taper and a 1:50 over the diameter of that boss, it comes to not very much. Better to have the correct taper of course, but given how beaten up that taper pin was, I would question whether it would even be noticed.

  3. #48
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    Really nice work Phil, I have only just come across this thread, I have no idea how I have missed it, but mis it I did. Thank you so much for the write up and all the great photos and captions. That alone would have taken me as long as the complete job took you. I just love how this forum brings so many helpful souls together, to come up with solutions to problems, or just another take on a problem. We all learn so much from the shared experience. As an aside, would there likely be any issues with Loctite losing strength at the operating temperatures of steam equipment such as this governor. Cheers,
    Rob

  4. #49
    Join Date
    Sep 2011
    Location
    Ballarat
    Age
    65
    Posts
    3,103

    Default

    Quote Originally Posted by Michael G View Post
    Phil, I have a collection of imperial pin reamers from 0 up to 5 I think. Would you like me to put one in the post so you can correct this 'grievous error'?

    Michael

    PS - if you calculate the difference in diameter between a 1:48 taper and a 1:50 over the diameter of that boss, it comes to not very much. Better to have the correct taper of course, but given how beaten up that taper pin was, I would question whether it would even be noticed.
    Hi Michael
    highly unlikely anyone would notice (though I would) plus I'm close to the largest pin I would like to put in in this situation plus thinking about how hard someone is likely to hit it down the track with a hammer worries me. Damn Metric.
    Even though the pin has been upsized it would have been nice if it was Imperial (it's driving me insane). If it is not too much trouble a #1 and #2 in the post would be fantastic as I still have a little 'wriggle room' left. Many thanks.

    Quote Originally Posted by Ropetangler View Post
    Really nice work Phil, I have only just come across this thread, I have no idea how I have missed it, but mis it I did. Thank you so much for the write up and all the great photos and captions. That alone would have taken me as long as the complete job took you. I just love how this forum brings so many helpful souls together, to come up with solutions to problems, or just another take on a problem. We all learn so much from the shared experience. As an aside, would there likely be any issues with Loctite losing strength at the operating temperatures of steam equipment such as this governor. Cheers,
    Rob
    Hi Rob
    I think a lot of you blokes are just being nice. My noggin is big enough.
    I would think that Loctite would be ok but I guess I'll never find out. I have certainly removed enough of the stuff over the years. Sadly I agree it certainly has a place in industry just not at my place.

    Phil

  5. #50
    Join Date
    Oct 2008
    Location
    N.W.Tasmania
    Posts
    1,407

    Default

    Quote Originally Posted by Steamwhisperer View Post
    Hi Michael
    highly unlikely anyone would notice (though I would) plus I'm close to the largest pin I would like to put in in this situation plus thinking about how hard someone is likely to hit it down the track with a hammer worries me. Damn Metric.
    Even though the pin has been upsized it would have been nice if it was Imperial (it's driving me insane). If it is not too much trouble a #1 and #2 in the post would be fantastic as I still have a little 'wriggle room' left. Many thanks.


    Hi Rob
    I think a lot of you blokes are just being nice. My noggin is big enough.
    I would think that Loctite would be ok but I guess I'll never find out. I have certainly removed enough of the stuff over the years. Sadly I agree it certainly has a place in industry just not at my place.

    Phil
    Thanks for the response Phil, but I have to say, Loctite has a pretty big future at my place

Page 4 of 4 FirstFirst 1234

Similar Threads

  1. Machining job needed - any takers?
    By Clinton1 in forum METALWORK GENERAL
    Replies: 4
    Last Post: 3rd Jun 2013, 08:41 PM
  2. Urgent machining job needed in perth.
    By lather in forum METALWORK GENERAL
    Replies: 2
    Last Post: 22nd Feb 2012, 07:08 PM
  3. aluminium machining advice needed
    By horse in forum METALWORK GENERAL
    Replies: 1
    Last Post: 12th Jan 2010, 02:10 PM
  4. Hercus 260ATM Install & Initial Setup Details Needed
    By jackafrica in forum THE HERCUS AREA
    Replies: 10
    Last Post: 28th Sep 2009, 07:34 PM
  5. Machining Needed in Sydney - low volume/prototype
    By missionaryman in forum METALWORK GENERAL
    Replies: 5
    Last Post: 29th Jan 2006, 08:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •