Failing incandescent bulb trips circuit breaker
I've recently had a maybe 2 year old ordinary 60W household light bulb trip the fuse box circuit breaker when it failed.
Normally when an incandescent bulb fails there is a break in the filament and that's that, no overheating, no excess current draw.
This bulb had obviously got quite hot, the inside of the glass was discoloured, it was grey and smoky. To me this is most unusual, what has likely happened here?
-
4th May 2016, 08:27 AM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Most incandescent bulb filaments break when they are switched of. The filament breaks because over time the metal slowly evaporates making it thinner and more brittle. On cooling the thinned out brittle filament cannot handle the tension from contraction and so it snaps. If it breaks when it is on and the gap is small it can sustain an arc like welder for a brief period. The arc is a plasma so instead of a few free electrons in the metal carrying a current now you have a ball of ionised metal gas and a many more freed electrons. This has a very low resistance so can carry hundreds or millions of amps (eg lightning) this will be more than enough to cause what you observed. Sometimes Thi happens when the globe is switched on because the filament is cold so has a lower initial resistance.
Similar Threads
-
Failing Vision
By beer4all in forum WELDINGReplies: 6Last Post: 15th Oct 2013, 01:26 AM -
A question regarding failing vision
By Grandad-5 in forum WELDINGReplies: 30Last Post: 29th Jul 2011, 12:57 AM -
Circuit Breaker- How Many Amp's?
By DirtPig in forum WELDINGReplies: 9Last Post: 26th Jul 2011, 12:32 AM -
200 amp arc welder (newb) why is my breaker always fliping?
By iceman423 in forum WELDINGReplies: 10Last Post: 28th May 2009, 09:26 PM -
Eye Sight Failing...Getting Old
By stevew in forum METALWORK GENERALReplies: 7Last Post: 10th Dec 2006, 09:32 PM