I am welding back together and adding brackets etc on a small ute tub.
It was originally .8mm but would now be .5 or less thanks to rust and panel work.
I have done plug welds with the mig in thicker spots but I’m afraid I’ll blow huge holes in this spot.
I have 15amp pp if needed.
The reach needed is only a bit over 150mm.
Thanks H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
30th Jan 2023, 09:36 AM #2I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,295
If you're wanting a spot welder, I assume you have access to the backside of the weld, so you could use a piece of copper bar/plate as a backer strip to take up some of the heat when using the mig...
I've found the spot welder can be pretty finicky when you don't have clean virgin material at times (ie: as likely to make holes as to weld, or not weld together due to tiny air gaps), but mine is just an el cheapo....
-
30th Jan 2023, 12:10 PM #3Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Portable 240v handheld spot welder Sydney
I agree. Copper backing bar works well for that sort of work - or for filling up old fastener holes in panels.
Edit: I’ve found using a flattened piece of 1/2” copper pipe works well to get into less accessible spaces.
Another option would be an adhesive sealant like one of the Sikaflex ones. They a damn strong if you have the appropriate joint situation and have the advantage of sealing up the joint to prevent it rusting again from the inside.
Steve
-
30th Jan 2023, 05:35 PM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I've a cheapo unit also, used mainly for spotting 1.2 galv sheet, without a timer
The arms can be reasonably deep, making it awkward to get in behind some panels. Also as J&H mentioned they can be VERY finicky even with clean virgin material.
KrynTo grow old is mandatory, growing up is optional.
-
1st Feb 2023, 07:08 AM #5
Thanks for the replies guys I had a mate from a nearby suburb lend me his el cheapo and it worked fine.
As a matter of fact it was easier for a mug to use than the real deal 3 phase unit my mates the auto body fabricators have. Their machine has multiple different heads which enables one to reach most areas but the extremely heavy cable and my age and damage to both shoulders made using it a major struggle whilst reattaching the tub chassis locators etc whilst working in their workshop.
I fugged up welding in one of the inner guards and on getting it home decided to redo it, so I had a few plug welds to do anyway after drilling out previous welds, I have various bits of copper backup scrap and spray areas to be welded with copper spray.
I might put some photos up in the car resto area.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
Similar Threads
-
Info on Pulsamatic spot welder
By Gaz99 in forum METALWORK GENERALReplies: 0Last Post: 21st Feb 2022, 09:23 PM -
Spot Welder Found on Ebay
By chambezio in forum METALWORK GENERALReplies: 3Last Post: 7th Jan 2017, 02:23 PM -
Spot welder question
By INVENTOR in forum WELDINGReplies: 3Last Post: 15th Jul 2016, 06:41 PM -
DIY spot welder questions
By jhovel in forum WELDINGReplies: 13Last Post: 24th Mar 2013, 12:46 AM -
Spot Welder
By Keith_W in forum WELDINGReplies: 4Last Post: 5th Apr 2009, 09:16 PM