    Hey guys.

    If anyone has brass or copper chips from machining that are clean I would love to buy them from you.

    Even titanium and alloy or bronze

    I have been casting the limited amount I have into resin for my knifemaking endeavours.

    Here is a pic of the end result.20220402_141004.jpg

    Sent from my SM-G998B using Tapatalk

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,958

    Default

    I got a heap from my local M10 from their key cutting machine, it is mixed with aluminium, but should still make a nice effective handle.
    If you're prepared to do some filing find some old brass taps and using a course file and some newspaper under the vise, file away to your hearts content.
    HTH
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Apr 2019
    Location
    Salisbury, South Australia
    Age
    38
    Posts
    29

    Default

    Quote Originally Posted by KBs PensNmore View Post
    I got a heap from my local M10 from their key cutting machine, it is mixed with aluminium, but should still make a nice effective handle.
    If you're prepared to do some filing find some old brass taps and using a course file and some newspaper under the vise, file away to your hearts content.
    HTH
    Kryn
    That's not a bad idea check some locksmiths. They don't run coolant to cut keys.

    I'm more looking for chips than filings. I have also cast filings in resin. Just not the same effect. And it tends to get dry spots no matter how much you stir it up. I wonder if a power rasp would make a larger filing that would work.



    Sent from my SM-G998B using Tapatalk

  4. #4
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,958

    Default

    Instead of a course file you could try a rasp or a Farriers file, they are VERY course for trimming horses hooves.
    I don't think a power file will do the trick as they are more of a sander and give fine pieces.
    Kryn
    To grow old is mandatory, growing up is optional.

  5. #5
    Join Date
    Jun 2007
    Location
    Ipswich QLD
    Age
    68
    Posts
    1,997

    Default

    Where are you located? Postage could be costly.

    Sent from my SM-T580 using Tapatalk

  6. #6
    Join Date
    Apr 2018
    Location
    Perth
    Posts
    168

    Default

    have you tried a local scrap metal dealer.
    I often see 44 gal drums of brass / bronze swarf in their yard.

Similar Threads

  1. Heavy wall brass or copper pipe
    By China in forum WANTED TO BUY
    Replies: 5
    Last Post: 29th Jan 2020, 03:13 PM
  2. Small square of brass or copper
    By racingtadpole in forum WANTED TO BUY
    Replies: 4
    Last Post: 28th Jan 2020, 08:31 PM
  3. Replies: 28
    Last Post: 4th Dec 2016, 02:33 PM
  4. Supplier for thin (4-6mm OD) copper or brass tubing
    By StevenManos in forum METALWORK GENERAL
    Replies: 6
    Last Post: 7th Jun 2016, 09:02 AM
  5. Brass/Copper finish
    By cookie48 in forum METALWORK GENERAL
    Replies: 2
    Last Post: 7th Jul 2011, 09:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •