Thanks: 0
Results 1 to 15 of 17
Thread: WTB - six step pulley???
-
30th Jan 2021, 11:24 PM #1New Member
- Join Date
- Jul 2015
- Location
- Blue Mountains
- Posts
- 5
WTB - six step pulley???
Hi all,
apologies for my first post being a request but I am in search of a six step alu pulley for my newly acquired Richardson E39 Drill press.
¾ bore.
the old one has fractured and has clearly been repaired multiple times already over its lifetime.
I found a four step option but I would really like to keep original if at all possible and find a six step.
I have tried most, if not all suppliers I can find with no success
thanks for any help.
Kai
-
31st Jan 2021, 06:49 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
Welcome to the forum.
There might be one out there but I would not count on it. Best options are to either repair the one you have or make up a new one from scratch. If you have not got a welder that can do Al or a lathe of sufficient swing, there are members here who can help.
Pictures of the item and some basic dimensions would help, as if someone does have a 6 step sitting around they willl be able to see if it is what you need.
Michael
-
31st Jan 2021, 09:28 AM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Just a heads up that not just any 6 step pulley can be used.
Firstly the V belt grooves needs to match up with the existing ones, as do the diameters, otherwise you may have to change the belt length every time you change belt pulley positions as there may not be enough adjustment available on the DP. If you cannot find one, or repair the exiting, or get one made then a single (intermediate) pulley a 3P Motor and a VFD would at least get you going.
-
31st Jan 2021, 09:59 PM #4New Member
- Join Date
- Jul 2015
- Location
- Blue Mountains
- Posts
- 5
Thanks for the replies.
Here are some pics of my current pulley ...AAE70A20-3246-43BE-96A3-014039A613E7.jpgC6C13306-0B68-4C6D-AA64-6214D1F0481F.jpgCC6EF744-283C-4F6D-B551-24CB0B902A40.jpg
-
31st Jan 2021, 10:43 PM #5
Hi Kaiser 63
Welcome to the MetalWork Forums,
To help you explore the other areas of our forum here's a guide on to to navigate our Forum and find all of our interesting places.
Goto the FORUM box in the top left hand cnr of the page and click ton it. This will bring up a pull down menu that has Forum Home at the top line.
Click Forum Home which will present a scroll down page.
Our rules,the Terms of Service are right at the top ,we encourage you to read them.They guide our behavior and conduct on the Forum/s.
Below that are all the various areas and sub forums that make up out MetalWork forums.
I'll leave the comment on your pulley to others with far more knowledge and experience than I.
Welcome to the MetalWork Forums
Grahame
-
1st Feb 2021, 07:07 AM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
Thanks for the pictures. That thing has cracks all over it, so while it could be welded up, I would suggest that the time and effort to do so would be excessive. There also looks to be two parts to that pulley - not sure whether it is original or not.
My suggestion would be to turn a new one up out of Al. Not a difficult task with the right tools.
Michael
-
2nd Feb 2021, 08:34 AM #7Golden Member
- Join Date
- Aug 2015
- Location
- Melbourne, Australia
- Posts
- 843
if I can make a multi-step pulley, seriously, anybody can. In the end it wasn't that hard, but I did have to spend some time on spreadsheeting measurements and so on, and nibbling away at something that large on my lathe.
https://metalworkforums.com/f65/t205...89#post1973089
-
2nd Feb 2021, 10:45 PM #8New Member
- Join Date
- Jul 2015
- Location
- Blue Mountains
- Posts
- 5
Thanks for the responses.
Yes, it’s had a hard life apparently...
Evidently it’s been repaired and modified to prolong its life by the previous owner who did a very good job considering. Yes it’s made up of three parts which vary in size a little
Having no luck so far with suppliers. It seems no one does 6 step anymore.
I will try and measure up the existing pulley at the quill side and look to have another made up maybe.
-
3rd Feb 2021, 07:37 AM #9Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
If you haven't got a lathe that will do it, there are a number of members here that could make up another for you. Probably cost you postage both ways (they would want the original to copy) and some material (and maybe something for time). I could do it for example, but there is likely someone closer.
Probably a cheaper option than going to a commercial machine shop.
Michael
-
9th Feb 2021, 09:43 PM #10China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Six step pulleys are not hard to find maybe you should check your post on WWF
-
9th Feb 2021, 10:04 PM #11New Member
- Join Date
- Jul 2015
- Location
- Blue Mountains
- Posts
- 5
Hi China,
thanks for that. Yes, I have been monitoring both threads for suggestions.
I have contacted all possible suppliers I have been suggested with no success.
this has included:
- HAFCO
- Blackwoods
- Australian Pulley co - Windsor
- Applied industrial - penrith
- Buttsworth
- Chain and drives
- Naismith
- BSC - Brisbane
- Ballarat bearings
- Lewis pulleys
- BIS - Vic
happy to take any new leads you may have?
otherwise I am looking at DIY at the moment.
-
9th Feb 2021, 10:57 PM #12China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
As I posted in WWF Royce Cross
-
10th Feb 2021, 09:35 AM #13New Member
- Join Date
- Jul 2015
- Location
- Blue Mountains
- Posts
- 5
Hi China, Yes thanks for that.
I did try them actually. I missed them in my list above. No luck. Best they can offer is a 4 inch, 4 step pulley.
Also tried Adelaide belt and hose. No options either.
Thank you though.
Looks like DIY is my only option at the moment.
-
10th Feb 2021, 03:33 PM #14China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Ok fair enough they list hem on their website, but as we know websites quite often do not tell the truth.
-
13th Feb 2021, 08:01 AM #15Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Are you still looking to buy?
Similar Threads
-
Sheraton 9'' model A counter shaft step pulley
By tharindu in forum WANTED TO BUYReplies: 0Last Post: 4th Jun 2020, 08:46 PM -
WTB 5 Step pulley
By kenny_10 in forum WANTED TO BUYReplies: 0Last Post: 17th Jun 2019, 02:25 PM -
Waldown 4 Step Motor Pulley
By Anorak Bob in forum METALWORK - Machinery, Equipment, MARKETReplies: 3Last Post: 19th Nov 2018, 03:57 PM -
How to make this? Maybe a step by step idiots guide please!
By ventureoverland in forum METALWORK GENERALReplies: 22Last Post: 19th Jul 2014, 08:02 PM -
Step by step on making a Square to Round transition
By Al B in forum METALWORK GENERALReplies: 34Last Post: 19th Sep 2012, 11:32 AM